Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 13.4 GPa | 1940 ksi | ASTM D638 |
Premix Premi-Glas® 3101-25 Polyester BMC Premi-Glas® 3101-25 is a 25% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL .. |
|||
Tensile Modulus | 13.4 GPa @Temperature 23.0 °C |
1940 ksi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Tensile Modulus | 13.4 GPa @Temperature 23.0 °C |
1940 ksi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Tensile Modulus | 13.4 GPa | 1940 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan.. |
|||
Tensile Modulus | 13.4 GPa @Temperature 23.0 °C |
1940 ksi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Tensile Modulus | 13.4 GPa | 1940 ksi | ASTM D638 |
Plenco 6310 Phenolic, Granular, Compression Molded PLENCO 06310 is a glass and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. 06310 is available in black.Information supplied by Plenco. |
|||
Tensile Modulus | 13.4 GPa | 1940 ksi | 1mm/min; ISO 527 |
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Conditioned) Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil.. |