Mechanical Properties Metric English Comments
Tensile Modulus 7.70 GPa
1120 ksi
Plastcom SLOVALEN PH 69 GF 45 PP, 45% glass fibre
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 45% glass fibre, contains the modifier of mechanical properties.Thermo stable. Increased strength in comparison wit..
Tensile Modulus 7.70 GPa
1120 ksi
ASTM D638
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Tensile Modulus 7.70 GPa
1120 ksi
ISO 527-1,2
Qualchem Danamid FGFLX2-30 Polyamide 6, 30% Glass Fiber
Reinforced with glass fiber. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt.
Tensile Modulus 7.72 GPa
1120 ksi
21% Glass Spray-up Laminate
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Tensile Modulus 7.72 - 7.93 GPa
1120 - 1150 ksi
20% Glass Laminate
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Tensile Modulus 7.70 GPa
1120 ksi
LATI Latigray 82-02 CX/80 PA 12
Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Tensile Modulus 7.70 GPa
1120 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..
Tensile Modulus 7.71 GPa
1120 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem ATX202R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Tensile Modulus 7.71 GPa
1120 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Tensile Modulus 7.71 GPa
1120 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Tensile Modulus 7.74 GPa
1120 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 (Asia Pacific)
LNP* Thermocomp* RFB53XXZ is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.
Tensile Modulus 7.70 GPa
1120 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East)
Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod..
Tensile Modulus 7.72 GPa
1120 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT
LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity.
Tensile Modulus 7.75 GPa
1120 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL EM7430 PPE+PS
30% glass reinforced, high flow PPO. Automotive. Energy management material.
Tensile Modulus 7.70 GPa
1120 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
Tensile Modulus 7.70 GPa
1120 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East)
Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus ..
Tensile Modulus 7.75 GPa
1120 ksi
ISO 527
Polyram Polytron P30N11 Polypropylene, 30% Long Fiber Glass
A chemically coupled 30% long fiber glass reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram.
Tensile Modulus 7.72 GPa
1120 ksi
21% Glass Spray-up Laminate
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Tensile Modulus 7.72 - 7.93 GPa
1120 - 1150 ksi
20% Glass Laminate
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Tensile Modulus 7.75 GPa
1120 ksi
ISO 527
Polyram Polytron P30B07 Polypropylene, 30% Long Glass Fibers, UV Stabilized
A chemically coupled 30% long glass fibers reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Tensile Modulus 7.75 GPa
1120 ksi
ASTM-D790
Polyram Polytron P30N01 Homopolymer Polypropylene, Chemically Coupled 30% Long Fiber
A CHEMICALLY COUPLED 30% LONG FIBER GLASS REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Tensile Modulus 7.72 GPa

@Temperature -20.0 °C
1120 ksi

@Temperature -4.00 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..
Tensile Modulus 7.70 GPa
1120 ksi
1mm/min; ISO 527
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and ..
Tensile Modulus 7.75 GPa

@Temperature -35.0 °C
1120 ksi

@Temperature -31.0 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..
Tensile Modulus 7.75 GPa
1120 ksi
Radici Radilon® A RV300R (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Tensile Modulus 7.75 GPa
1120 ksi
ASTM-D790
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF
A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Tensile Modulus 7.75 GPa
1120 ksi
ASTM-D790
Polyram Polytron P30B11 Homopolymer Polypropylene, Chemically Coupled 30% LGF
A chemically coupled 30% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind.