Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
PolyOne Nymax™ GMF 604 40 UV Black 148 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | TM R050-36 |
Resinlab® EP1330 Heat Cure Epoxy Polymer System Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-NP-110-W-NAT Polyamide 12 (Nylon 12) Information provided by PolyOne |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
PolyOne Nymax™ X GMF 604 40 UV Black 148 rev 4 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties) Description:#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 per.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific) LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific) LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.27 GPa @Temperature -60.0 °C |
1200 ksi @Temperature -76.0 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Ensinger Tecatron® XP-68 Compression Molded PPS Compound, 25% Fiberglass with Graphite Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PI-20GM-20CF/000 Polyetherimide (PEI), Carbon/Glass Filled
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedCarbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Solvay Specialty Polymers Parmax® 1200 Self-Reinforcing Polyethersulfone
(discontinued **) PARMAX 1200 self-reinforcing polymer (SRP) is an ultra-high performance amorphous, melt-processable engineering thermoplastic. The unique properties of this material are due primarily to the inheren.. |
|||
Tensile Modulus | 8.27 GPa | 1200 ksi | ASTM D638 |
Plenco 6554 Phenolic, Granular, Compression Molded
(discontinued **) Two-Stage Phenolic. PLENCO 06554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 06554 is available in black.Information supp.. |