Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.69 GPa @Temperature 100 °C |
970 ksi @Temperature 212 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Tensile Modulus | 6.69 GPa | 970 ksi | Conditioned; ASTM D638 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Tensile Modulus | 6.69 GPa | 970 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC STAMAX 30YM240 PP SABIC® STAMAX 30YM240 is a 30% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16496906... |
|||
Tensile Modulus | 6.69 GPa | 970 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD.. |
|||
Tensile Modulus | 6.69 GPa @Temperature 100 °C |
970 ksi @Temperature 212 °F |
2; ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry) Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Tensile Modulus | 6.69 GPa | 970 ksi | ASTM D638 |
Asahi Kasei Thermylene® P6-43FG-0410 43% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |