Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Oxford Polymers 10GF 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 5.86 GPa @Temperature 22.8 °C |
850 ksi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PS-15GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet) Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI .. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ NL-15CF-15GF/5M Nylon 6/12, Carbon/Glass Filled
(discontinued **) Description/Features:Carbon Fiber ReinforcedGlass Fiber ReinforcedMolybdenum Disulfide LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30 Polypropylene Homopolymer, 30% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30/E3 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30/E4 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30/E8/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4702-15 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | |
Abatron AboCast/AboCure 8502-1 Epoxy AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v.. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® ES-20GF/000 Polyethersulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |