Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4701-30-20 Supported Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Contains PET film reinforcement.Features and Benefits of PORON Products: Excellent compression set resistance which ena.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | MD, supporting material; ASTM D882 |
Rogers Corporation Poron® Shock Seal™ 4790-79-9 Handheld Urethane Foam, Handheld Grade, PET Reinforced Extreme Impact Protection, Ultimate ReliabilitySpecifically engineered to protect sensitive components from damage caused by impactConsistent cushioning performance through repeated impactsExcellent.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | |
Radici Radiflam® S AE (dry) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | >= 3.45 GPa @Temperature 23.9 °C |
>= 500 ksi @Temperature 75.0 °F |
|
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation .. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | |
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy Description: Master Bond Polymer Compound EP45HTQ is a two component quartz filled, epoxy compound for high performance structural bonding and casting. It is suitable for applications where long ter.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | |
Master Bond EP33ND Epoxy Paste Resists Harsh Chemicals Description: Master Bond EP33ND is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g.. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ MP-10GF/10T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 3.45 GPa | 500 ksi | ASTM D638 |
Quantum PEEK Information provided by Quantum Advanced Engineering Plastics |