Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.30 GPa | 479 ksi | |
Polycasa Acryl® G 88 Acrylic Glazing, domed roof lights, lighting covers, publicity lighting, reflectors, lenses, instrument covers, dishes and bowls; mostly used in the automotive industry.Data was collected by ISO methods.Qui.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 505R PC (Asia Pacific) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP FARADEX NX96302 PC+ABS LNP* FARADEX* NX96302 is a compound based on PC+ABS resin containing Stainless Steel Fibers. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP CGI11XP PS (Europe-Africa-Middle East) LNP* Lubricomp* CGI11XP is a compound based on Polystyrene resin containing Graphite. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527 |
Polycasa CAST PMMA QUINN CAST has an optical transparency of 93% light transmission for transparent sheets. It is significantly lighter and much more impact resistant than glass of equivalent thickness. QUINN CAST is .. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527 |
Nilit FRIANYL B63 W-KV10 Nylon 6 for injection molding, 10% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.30 GPa @Temperature 23.0 °C |
479 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1mm/min; ISO 527 |
Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. High stiffness and flowability realize the thin wall of large-scale business machine chassis.Information provided by Tei.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527 |
Styrolution PS 165 N/L GPPS Styrolution PS 165N/L is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.High molecular weightGood flow characteristicsAppropriate for blending with HIPS.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1mm/min; ISO 527-2 |
Borealis MG302Al Polypropylene Compound, Mineral Filled MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt .. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TS300 PA46 |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
DSM Stanyl® TW341 (DAM) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | dry; ISO 527-1/-2 |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
DSM Stanyl® TW441 (DAM) Nylon 46 High Viscosity, Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | |
BASF Polystyrol® 158 K Polystyrene (Global) Heat-resistant, rapid freezing general-purpose grade. Suitable for expanded film and for blending with Styrolux and impact-modified Polystyrol in heat contact applications (e.g. coffee cups).Data w.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | 1 mm/min |
Arkema Group Altuglas® 84 L Acrylic-Styrene Copolymer ALTUGLAS 84 L is a new type of acrylic polymer produced by ATOHAAS which increases the range of material for injection molding applications. ALTUGLAS 84 L is a styrene methylmethacrylate copolymer s.. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TS FR PA666 FR Information provided by EMS Grivory |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |
|||
Tensile Modulus | 3.30 GPa | 479 ksi | ISO 527 |
Grupo Repol Dinalon® B2S35 V2-7035 PA6 High Viscosity, V2 Halogen Free, RAL 7035 Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |