Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA)
(Unverified Data**) Ixef 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1025/9.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ASTM D638 |
Glastic BMC SLC-1000 Glass-Reinforced Polyester Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 9945 HFFR Polyamide, High Performance (HPPA), 45% Glass Fiber Kalix® 9945 HFFR is a 45% glass-fiber reinforced, halogen-free flame retardant High Performance Polyamide. It is hot-water moldable and intended for use in components requiring superior mechanica.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-2 |
Solvay Specialty Polymers Omnix® FC-9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® FC-9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific) LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ASTM D638 |
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527 |
Vyncolit X620/1 Novolac Phenolic Glass fiber and graphite filled phenolic molding compound with excellent friction properties.USES: Low friction bearings, video recorder and compact disc parts. Not suitable for applications requir.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | 90º, RT, Dry; EN2561 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 63%/120 E-Glass Fiber Information provided by HexCel |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® 1SVX-65H nat PA1010-GF65 Product Description: Grilamid 1SVX-65H natural is a 65% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5H black PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H FWA black 9225 PA12-GF65 Product description: Grilamid LV-65H FWA black 9225 is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-65H FWA nat PA12-GF65 Product description: Grilamid LV-65H FWA natural is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50 Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | 1 [mm/min]; ISO 527-2/1 |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | ISO 527-1 |
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited fo.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Modulus | 17.0 GPa | 2470 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVX-5 H black 9915 PA*-GF50 Product description: Grivory GVX-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |