Polymer Property : Tensile Modulus = 15.4 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 15.4 GPa
2230 ksi
LATI Latiohm 62-03 PD01 G/20 PPA, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 6 (PA6). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust..
Tensile Modulus 15.4 GPa

@Temperature 100 °C
2230 ksi

@Temperature 212 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Tensile Modulus 15.4 GPa
2230 ksi
ISO 527-2
Solvay Specialty Polymers Amodel® FC-1140 Polyphthalamide (PPA), 40% Glass Fiber
Amodel® FC-1140 is an FDA-approved, 40% glass fiber reinforced resin designed for high strength and stiffness. This combines with its excellent thermal properties, low water absorption and good h..
Tensile Modulus 15.4 GPa
2230 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp RF00ASXP PA6.6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RF00ASXP is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi..
Tensile Modulus 15.4 GPa
2230 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East)
LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.
Tensile Modulus 15.4 GPa
2230 ksi
1 mm/min; ISO 527-1
Sax Polymers SAXAMID 126F10 Nylon 6, 50% Glass Fiber
SAXAMID 126F10 is a polyamide 6 injection-molding-grade reinforced with 50% glass fibers.Information provided by SAX Polymers
Tensile Modulus 15.4 GPa
2230 ksi
ASTM D638
Plenco 6015 Phenolic, Briquette, Injection Molded
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf..
Tensile Modulus 15.4 GPa
2230 ksi
1 mm/min; ISO 527
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded
Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar.
Tensile Modulus 15.4 GPa
2230 ksi
1 mm/min; ISO 527
Eurostar Staramide RF00ASXS PA66, 50% Glass Filled, Injection Molded
Staramide RF00ASXA is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Tensile Modulus 15.4 GPa

@Temperature 100 °C
2230 ksi

@Temperature 212 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..