Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.3 GPa | 1500 ksi | ASTM D638 |
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
Tensile Modulus | 10.3 GPa | 1500 ksi | tangent; ASTM D638 |
Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: Compatible with in-mold coatings,.. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | Lengthwise/Crosswise; ASTM D-638 |
Glastic 1130 Angles, Channels, and Structural Shapes Information provided by Glastic Corporation |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F7 Nylon 6, 35% Glass Fiber SAXAMID 126F7 is a polyamide 6 injection-molding-grade reinforced with 35% glass fibers. Because of its high strength and stiffness this grade is often used for stressed parts. Additional properties.. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 25378 Phenolic, Compression Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | ASTM D638 |
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | ASTM D638 |
Plenco 1501 Polyester, Pellet, Injection Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Tensile Modulus | 10.3 GPa @Temperature -40.0 °C |
1490 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d.. |
|||
Tensile Modulus | 10.3 GPa | 1500 ksi | ASTM D638 |
Applied Composites 8022 Polyester SMC Industry Application: ConstructionProduct Application: Water TreatmentDistinct Features: Ideal for Buried Applications, Construction, High Corrosion Resistance in Waste Water Treatment, Dimensional .. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Modulus | 10.3 GPa | 1500 ksi | 45° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Tensile Modulus | 10.3 GPa | 1490 ksi | Lengthwise/Crosswise; ASTM D-638 |
Glastic GLASGUARD 1130 Corrosion-Resistant Panels GlasGuard Grade 1130 is a fiberglass-reinforced thermoset polymer composite system which is available as sheet stock or in a variety of pultruded shapes. Grade 1130 possesses flame resistance, corr.. |