| Category | Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS |
| Manufacturer | Glastic |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Glastic 1130 Angles, Channels, and Structural Shapes.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Water Absorption | 0.10 % | 0.10 % | % by wt.; ASTM D-570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 101 MPa | 14600 psi | Lengthwise; ASTM D-638 |
| 110 MPa | 16000 psi | Crosswise; ASTM D-638 | |
| Tensile Modulus | 10.3 GPa | 1490 ksi | Lengthwise/Crosswise; ASTM D-638 |
| Flexural Strength | 141 MPa | 20400 psi | Lengthwise; ASTM D-790 |
| 161 MPa | 23300 psi | Crosswise; ASTM D-790 | |
| Flexural Modulus | 9.58 GPa | 1390 ksi | Crosswise; ASTM D-790 |
| 9.72 GPa | 1410 ksi | Lengthwise; ASTM D-790 | |
| Adhesive Bond Strength | 42.1 MPa | 6100 psi | lbs.; NEMA 11.11 |
| Izod Impact, Notched | 6.03 J/cm | 11.3 ft-lb/in | ASTM D-256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | V-0 | V-0 | |
| Flame Spread Index | 12 | 12 | Radiant Panel; ASTM E-162 |
| 20 | 20 | UL Standard 723; ASTM E-84 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 12.4 kV/mm | 315 kV/in | Perpendicular S/T in Air; ASTM D-149 |
| Arc Resistance | 192 sec | 192 sec | ASTM D-495 |
| Track Resistance | 52200 sec | 52200 sec | Inclined Plane; ASTM D-2303 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Electric Strength kV, ASTM D149 | 75 | Parallel, Condition A |
| 79 | Parallel, Condition D (48/50) | |
| Smoke Developed | 115 | ASTM E-84 |
| Standard Color | Gray | |
| UL Recognition File Number | R9599 | |
| UL Standard 723 Fuel Contributed | 0 | ASTM E-84 |