Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.94 GPa | 281 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Modulus | 1.94 GPa | 281 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Asia Pacific) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 1.94 GPa | 281 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS LNP LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 1.94 GPa | 281 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL002 ABS (Europe-Africa-Middle East) LNP* LUBRICOMP* AL002 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 1.94 GPa | 282 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.94 GPa | 282 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 1.94 GPa | 281 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® XLG2400 PC+PET Low Gloss Xenoy, providing inherent low gloss on almLow Gloss Xenoy, providing inherent low gloss on almost every type of tool surfaces. This grade has excellent low temperature impact, high heat re.. |
|||
Tensile Modulus | 1.94 GPa | 281 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact Applications Zytel FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food .. |
|||
Tensile Modulus | 1.94 - 2.25 GPa | 281 - 326 ksi | ASTM D638 |
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor.. |
|||
Tensile Modulus | 1.94 GPa | 281 ksi | 1 mm/min |
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp.. |
|||
Tensile Modulus | 1.94 GPa @Temperature -20.0 °C |
282 ksi @Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |