Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.26 GPa | 183 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Cellular E8202 Polyvinyl Chloride, Rigid (PVC, Rigid) All physicals were measured on an actual extruded part of a shutter profile.High rate inward foam applications.Density range .55-.70.Information provided by PolyOne |
|||
Tensile Modulus | 1.26 GPa | 183 ksi | 50 mm/min; ASTM D638 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Tensile Modulus | 1.26 GPa | 183 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber. |
|||
Tensile Modulus | 1.26 GPa | 183 ksi | Bar; ISO 527-3 |
Topas Advanced Polymers TOPAS® 9903D-10 Cyclic Olefin Copolymer (COC) TOPAS® 9903D-10 is a very low glass transition temperature (Tg=33°C) film extrusion grade. It is designed to deliver high shrinkage at low temperatures in shrink packaging applications. It is a mo.. |
|||
Tensile Modulus | 1.26 GPa | 183 ksi | 1 mm/min |
Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Conditioned) Designation ISO 1874-PA11,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Good chemical resistanc.. |
|||
Tensile Modulus | 1.26 GPa | 183 ksi | 1 mm/min |
Arkema Group Rilsan® BMN D Nylon 11 (Dry) Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d.. |
|||
Tensile Modulus | 1.26 GPa | 183 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON MS000IL PP LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c.. |