Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.260 GPa @Temperature 23.0 °C |
37.7 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | |
LyondellBasell Lupolen® 2420 F LDPE Film, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | |
LyondellBasell Lupolen® 2420 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | |
LyondellBasell Lupolen® 2420 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | |
LyondellBasell Lupolen® 2425 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | |
LyondellBasell Lupolen® 2426 F LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | |
LyondellBasell Lupolen® 2441 D LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific) LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | TD; ASTM D882-A |
Borealis FT5230 Low Density Polyethylene FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: .. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | TD; ASTM D882-A |
Borealis FT5231 Low Density Polyethylene FT5231 is a Low Density Polyethylene for blown film. Tubular technology. Contains Antioxidant. This grade is developed for the production of packaging film with good optical properties for medium d.. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | TD; ASTM D882-A |
Borealis FT5232 Low Density Polyethylene FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op.. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | TD; ASTM D882-A |
Borealis FT5236 Low Density Polyethylene FT5236 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes anti-block, antioxidant and medium slip additives. Applications FT5236 has been developed especially for applic.. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | ISO 527-1/-2 |
DSM Arnitel® EM631-HB TPC-ET Extrusion Grade, Heat Stabilized |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® SC969 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | MD |
BASF Ultramid® B32 0.015 BOPA Film Information provided by BASF |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | MD |
Kuraray HYBRAR® BF1 Three Layer Blown Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber w.. |
|||
Tensile Modulus | 0.260 GPa | 37.7 ksi | |