Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.250 GPa | 36.3 ksi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio.. |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Tensile Modulus | 0.250 GPa @Temperature 23.0 °C |
36.3 ksi @Temperature 73.4 °F |
|
LATI Lastane 50 PUR Polyurethane (PUR). Unfilled. Very good noise reduction. Good impact resistance even at low temperature.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | ISO 527-1/-2 |
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® ELX 40 HNZ TPA Product description: Grilon ELX 40 H NZ is a high viscosity, heat stabilized, impact modified, thermoplastic PA6 elastomer for extrusion blow moulding applications. Grilon ELX 40 H NZ has the follow.. |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | ISO 527 |
Eurotec® Tecomid® NB50 NL IT PA6, impact modified, super tough, natural, extrusion grade Information provided by Eurotec® |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | ISO 527-1/-2 |
DSM Arnitel® UM551-V Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | ISO 527-1/-2 |
DSM Arnitel® UM552 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | ISO 527-1/-2 |
DSM Arnitel® UM551-V 55 Shore D, Flame Retardant (halogen-, phosphorous-free) Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | |
Kuraray HYBRAR® PH3 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber w.. |
|||
Tensile Modulus | 0.250 GPa | 36.3 ksi | |
Henkel SynSpand 9835 Expanding Syntactic Film Expanding modified epoxy film, cures at 300°F / 149°C, used for jet engine abradable fan seals. |