Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 50.0 - 210 MPa | 7250 - 30500 psi | Average value: 111 MPa Grade Count:16 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Yield | 60.0 - 210 MPa | 8700 - 30500 psi | |
Materion Beryllium Copper Alloy 10 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 60.0 - 210 MPa | 8700 - 30500 psi | |
Materion Beryllium Copper Alloy 10 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 - 210 MPa | 18900 - 30500 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 - 210 MPa | 18900 - 30500 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 - 210 MPa | 18900 - 30500 psi | |
Materion Beryllium Copper Alloy 25 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 60.0 - 210 MPa | 8700 - 30500 psi | |
Materion Beryllium Copper Alloy 3 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 60.0 - 210 MPa | 8700 - 30500 psi | |
Materion Beryllium Copper Alloy 3 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 130 - 210 MPa | 18900 - 30500 psi | |
Materion Beryllium Copper Alloy M25 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 60.0 - 210 MPa | 8700 - 30500 psi | |
Materion Beryllium Copper Alloy 3 Tube; A (TB00) Temper; All Sizes (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |