Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 483 - 965 MPa | 70000 - 140000 psi | |
Meehanite Ductliron® AQS Nodular Graphite Ductile Iron Type AQS is an air hardening metal possessing high strength, toughness and hardness. It may be fully air quenched throughout casting section after machining to a wide range of strength and hardness.. |
|||
Tensile Strength, Yield | 758 - 965 MPa @Strain 0.200 % |
110000 - 140000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic.. |
|||
Tensile Strength, Yield | 896 - 965 MPa @Strain 0.200 % |
130000 - 140000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS03 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |