Material Notes:
Type AQS is an air hardening metal possessing high strength, toughness and hardness. It may be fully air quenched throughout casting section after machining to a wide range of strength and hardness values that are uniform with little or no risk of cracking or distortion. It has high endurance strength and provides an excellent degree of abrasion resistance.General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Mechanical Properties Metric English Comments
Hardness, Brinell 225 - 500
225 - 500
Nominal
Tensile Strength, Ultimate 552 - 1240 MPa
80000 - 180000 psi
Tensile Strength, Yield 483 - 965 MPa
70000 - 140000 psi
Elongation at Break 1.0 - 3.0 %
1.0 - 3.0 %
Modulus of Elasticity 172 GPa
25000 ksi
Fatigue Strength 365 MPa
53000 psi
Endurance Limit (Unnotched)
Thermal Properties Metric English Comments
Shrinkage 1.3 %
1.3 %
Patternmaker Shrinkage