Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 34.5 - 76.0 MPa | 5000 - 11000 psi | Average value: 51.4 MPa Grade Count:46 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Yield | 60.0 - 75.8 MPa | 8700 - 11000 psi | Average value: 63.0 MPa Grade Count:29 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Yield | 71.7 - 76.0 MPa | 10400 - 11000 psi | Average value: 74.4 MPa Grade Count:3 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Yield | 55.0 - 76.0 MPa | 7980 - 11000 psi | Average value: 69.5 MPa Grade Count:4 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Tensile Strength, Yield | 20.0 - 76.0 MPa | 2900 - 11000 psi | Average value: 39.5 MPa Grade Count:34 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Yield | 75.2 - 75.7 MPa | 10900 - 11000 psi | 90 Minute UV Cure + Thermal; ASTM D638 |
3D Systems Accura® SI 40 Plastic for the SLA® 250 System Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |
|||
Tensile Strength, Yield | 62.0 - 76.0 MPa | 8990 - 11000 psi | ASTM D638 |
3D Systems Accura® 10 Plastic for SLA® Systems Accura 10 "Nd" type material - for use with Viper SLA, and SLA 3500, 5000 and 7000 systems.ApplicationsGeneral use prototyping for many uses, including:Enclosures, covers and casesCellular/mobile ph.. |
|||
Tensile Strength, Yield | 20.0 - 75.8 MPa | 2900 - 11000 psi | Average value: 47.2 MPa Grade Count:46 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |