Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging PK8-1080 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87624 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5000 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M5015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AT-000/05T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AT-000/05T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-000/20T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Novablend™ 5035 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Therma-Tech™ NNC-5000 TC Polyamide 66 (Nylon 66) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® AT-000/000 HI5 Natural NA Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | |
Ineos ABS Lustran® 248 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | ASTM Data |
Styron Magnum™ 2610 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | ASTM Data |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 48.3 - 62.7 MPa | 7010 - 9090 psi | Average value: 55.7 MPa Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Yield | 48.3 MPa | 7010 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® XT XT-100-CX02-EG PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |