Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 41.3 MPa | 5990 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Strength, Yield | 41.3 MPa | 5990 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ HTX 92052 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Tensile Strength, Yield | 41.3 MPa | 5990 psi | |
Ineos ABS Lustran® 446 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Tensile Strength, Yield | 41.3 MPa | 5990 psi | ASTM-D638 |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Tensile Strength, Yield | 41.3 MPa @Temperature 23.0 °C |
5990 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H53N-00 Polypropylene Homopolymer This is a high flow rate nucleated and lightly lubricated homopolymer polypropylene designed for high-speed injection molding of thin-walled parts requiring good stiffness and fast cycle times. Thi.. |
|||
Tensile Strength, Yield | 41.3 MPa | 5990 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3500 ELG Natural 1003 Injection Molding Grade, High Flow, Medium Impact, Low Gloss Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 41.3 MPa | 5990 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3500 Natural 1003 Injection Molding Grade, High Flow, Medium Impact, Low Gloss Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 41.3 MPa | 5990 psi | chs 20 in/min; 300% elongation; ASTM D412 |
Diamond Polymers Softflex® 6538 Thermoplastic Elastomer Alloy, Clear Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |