Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 33.1 MPa | >= 4800 psi | ASTM D638-97 |
S&E Specialty Polymers GPP™ 1005M-EX10 Natural PP Application: UL94 V-2, Non-blooming flame-retardant polypropylene compound for injection moldingInformation provided by S&E Specialty Polymers |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-0216 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH120 Polypropylene, Homopolymer, Injection Molding, Barefoot Formulated for excellent processing stability. Applications: General purpose injection molding. Equivalent to Pro-fax® HL23INInformation provided by Phillips 66. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH200L Polypropylene, Homopolymer, CR, Antistat, Injection Molding COPYLENE™ CH200L is designed for general purpose injection molding applications with anti-static and controlled rheology. Applications: Food Containers, Housewares, Closures.Information provided by.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CH020-03 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020-03 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applicationsApplications: Bags & Pouches, Raffia/Tapes/Strapping, Peelabl.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CH020S Polypropylene, Homopolymer, BOPP COPYLENE™ CH020S is a polypropylene homopolymer resin typically used by customers for BOPP (biaxially oriented polypropylene) Applications: Film ExtrusionInformation provided by Phillips 66. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
M. Holland Company PP100 Polypropylene Homopolymer, General Purpose High clarityHomopolymerGood melt strengthHigh tensile strengthApplications: Thin-walled partsSheetStrapping |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Global TPP-120 20% Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Ineos N00N-00 Polypropylene Impact Copolymer Grade N00N-00 is a fractional melt flow rate, high impact copolymer polypropylene specifically designed for non-pressure structured wall pipe but can also be used in other extrusion applications req.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PP1-2001A Antimicrobial Polypropylene Homopolymer A 20 melt injection molding grade of Polypropylene homopolymer containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information pro.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Lucent Polymers TPP-120 Polypropylene, Homopolymer, 20% Talc Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Ineos N01N-00 Polypropylene Impact Copolymer Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properti.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Techmer ES HiFill® HDPE MM40 40% Mica Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mica Filler, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Spartech PP5312 Mica Reinforced Homopolymer Information provided by Spartech |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Techmer ES Plastiblend® ABS IM Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPallets.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 1103K Homopolymer Polypropylene Homopolymer for BOPP Film Formolene® 1103K is a high molecular weight, highly isotactic, polypropylene homopolymer designed for extrusion processes notably slit tape applications. It contains a uni.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite Butyrate 580A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D412 |
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This ne.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPP 200-4 PP Black Polypropylene Copolymer, No Break AAROLENE® ARPP 200-4 Series Polypropylene Compounded ResinFeatures: A copolymer polypropylene resin, pre-colored black, featuring excellent toughness for all extrusion applications. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D-638 |
Bapolene® 4072 Polypropylene, Injection Grade Bapolene PP4072 is a high flow, fast cycle injection molding resin. This product meets FDA standards for food contact applications.Applications: Appliances, containers, and thin-walled articles.Bap.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH014 Polypropylene, Homopolymer, Extrusion, Strapping COPYLENE™ CH014 is a polypropylene homopolymer resin designed for extrusion applications. Applications: Raffia/Tapes/Strapping; Geotextile & Agriculture; Nets. Equivalent to Pro-fax® HL781GInforma.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH016 Polypropylene, Homopolymer, BOPP COPYLENE™ CH016 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches; Raffia/Tapes/Strapping; Peelable.. |