Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527 |
Polimeri Europa Eraclene® BB 76 High Density Polyethylene - Blow Molding Eraclene BB 76 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 30 liters.Er.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
North Wood Plastics Polypropylene with 20% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | Extension rate 2 in/min; ASTM D638 |
NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffnessApplications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert a.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527 |
Polimeri Europa Eraclene® MS 80 High Density Polyethylene - Injection Molding Eraclene MS 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MS 80 shows a good balance between processability and mechanical pro.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
SABIC PP 623B Polypropylene Random Co-polymer for Cast Film Product Description: PP 623B is a PP Random Copolymer grade specially designed for Cast PP (CPP) film extrusion. It contains slip agent and anti-block additives. PP 623B offers good heat weldabil.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
Ineos Nova 5730 High flow, High impact
(discontinued **) High flow, High impact, USP Class VIApplications: Toys, Medical, HousewaresProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provi.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
Global R-1760 High Density Polyethylene, Injection Molding Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesMeets FDA requirements as listed in.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
Braskem ES 002G HDPE Pipe Extrusion Polyethylene
(discontinued **) Applications: Flat and corrugated pipes extrusion for mining, energy and telecommunication systems; piping in sewage systems. Information provided by Braskem |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
Flint Hills PP 23R2A Random Copolymer Polypropylene Random copolymer, radiation sterilization resistant, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliantFeatures: High contact clarity, non-blushing, toughness, impact, chemical.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638-02 |
Ipiranga Petrochem GF 5250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527 |
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse .. |
|||
Tensile Strength, Yield | 27.0 MPa @Strain 0.200 %, Temperature 1095 °C |
3920 psi @Strain 0.200 %, Temperature 2003 °F |
|
Haynes 214® alloy, cold rolled annealed sheet 2.0-3.2 mm thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate Key Features: fractional melt flow, medium high modulus, UV-stabilized, mineral-filled, blow molding and extrusion grade polypropylene copolymer, excellent impact and stiffness balance, good melt st.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527 |
Styrolution PS 476L HIPS Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | BP 13B/1 |
SIDPEC EGYPTENE® HD 5740 UA HDPE Injection Molding Applications:Large dustbins and pailsPallet boxesFish cratesTechnical moldingInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
Teknor Apex Sinpolene CPP2020 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 20% Filler by Weight Features: Copolymer Uses: Furniture Forms: PelletsInformation Provided .. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50mm/min; ISO 527-2 |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50mm/min; ISO 527-2 |
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer BorPure™ RE450MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is characterized by optimum combination of high impact strength and.. |
|||
Tensile Strength, Yield | 27.0 - 29.0 MPa | 3920 - 4210 psi | MD/TD; ISO 527-2 |
Borealis HB205TF Polypropylene HB205TF is a low melt flow rate polypropylene homopolymer intended for extrusion, calendering and thermoforming. Its very good organoleptic properties allows this grade to be used with any master b.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D 638 |
Cossa Polimeri ESTAPROP H 0360 T8 Polypropylene, 30% Mineral Filled PP homopolymer 30% mineral fillerExtrusion gradeInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D 638 |
Cossa Polimeri ESTAPROP HK 2540 T8 Polypropylene, 20% Mineral Filled PP homo/copolymer 20% mineral fillerGood physical and mechanical propertiesInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ CMU 101D Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior trim in which good surface finish, high scratch resistance, minimum dust deposit and good UV resistan.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 2 in per min; ASTM D638 Type IV |
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50 mm/min |
Arkema Group Rilsan® MA 4411 Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit fo.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | |
BASF Polystyrol® 455 F WU Impact Grade Polystyrene (Europe) Very easy-flowing, impact-modified grade.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527-1 |
Orbilan ORBILAN® PE 500 HMW-PE Orbilan PE 500 plastic is used as cutting boards for the food industry and gastronomy, in refrigeration chambers as ram protection and for swing doors as well as at sports grounds for sheets or hand.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ CMW 402 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive under-the-hood applications. Availability: Africa & Middle East, Asia Pacific, Europe, South America and North.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |