Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 260 MPa | 37700 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East) LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Tensile Strength, Yield | >= 260 MPa | >= 37700 psi | |
MetalTek 254 SMO® Super Austenitic Stainless Steel Corrosion resistance approaching nickel alloys, especially in chloride service. Produced under license of Avesta Jernverk AB. Applications: Process piping exposed to flue gas and solutions.Informati.. |
|||
Tensile Strength, Yield | >= 260 MPa | >= 37700 psi | |
MetalTek MTEK 6XN Cast UNS J94651 Super Austenitic Stainless Steel Corrosion resistance approaching nickel alloys, especially in chloride service.Applications: Process piping exposed to flue gas and solutions.Information provided by MetalTek |
|||
Tensile Strength, Yield | 260 MPa @Strain 0.200 % |
37700 psi @Strain 0.200 % |
|
Haynes 556® alloy, bar after 16000 hours at 537°C Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 260 MPa @Strain 0.200 % |
37700 psi @Strain 0.200 % |
|
Haynes 556® alloy, bar after 16000 hours at 648°C Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 260 MPa | 37700 psi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
Tensile Strength, Yield | 260 MPa @Strain 0.200 % |
37700 psi @Strain 0.200 % |
Annealed prior to test |
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a.. |
|||
Tensile Strength, Yield | 260 - 320 MPa @Strain 0.200 % |
37700 - 46400 psi @Strain 0.200 % |
|
SSAB Tunnplat Aluzink 260A RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink RP - rephosphorized steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.5 - 1.5 mm. Iron content is approximate - exact compo.. |
|||
Tensile Strength, Yield | <= 260 MPa @Strain 0.200 %, Thickness <=0.700 mm |
<= 37700 psi @Strain 0.200 %, Thickness <=0.0276 in |
20 MPa higher apply |
SSAB Tunnplat Aluzink F30A Metal-coated Mild Steel Metal-coated Mild SteelComments: Aluzink - Aluminum-zinc coated sheet. Property values are for thicknesses 0.4 - 2.00 mm. Iron content is approximate - exact composition is not reported by the manu.. |
|||
Tensile Strength, Yield | 260 - 320 MPa @Strain 0.200 % |
37700 - 46400 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 260 RP High-strength Steel High-strength SteelComments: Docol RP - Cold Rolled Steel - rephosphorized steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.0 mm. Iron content is approximate - exact compositi.. |
|||
Tensile Strength, Yield | 260 - 320 MPa @Strain 0.200 % |
37700 - 46400 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal 260 RP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Yield | 260 - 320 MPa @Strain 0.200 % |
37700 - 46400 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal 260 RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Yield | 260 - 330 MPa @Strain 0.200 % |
37700 - 47900 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal 260YP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur.. |
|||
Tensile Strength, Yield | <= 260 MPa @Strain 0.200 % |
<= 37700 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal F30 Metal-coated Mild Steel Metal-coated Mild SteelComments: Dogal - Hotdipped-galvanized sheet. Property values are for thicknesses 0.5 - 2.5 mm. Iron content is approximate - exact composition is not reported by the manufac.. |
|||
Tensile Strength, Yield | 260 MPa | 37700 psi | As Cast |
AFE Technologies Cronite 25Cr/20Ni No. HR6 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |
|||
Tensile Strength, Yield | 260 - 470 MPa @Strain 0.200 % |
37700 - 68200 psi @Strain 0.200 % |
|
ALIMEX PLANAL 7075 T651/T652 Aluminum Alloy Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi.. |
|||
Tensile Strength, Yield | 260 MPa | 37700 psi | |
ATI Allegheny Ludlum AL 304DA Stainless/Carbon Steel Three-Ply Composite Composition above represents only the Type 304 cladding. Its iron content calculated as balance.Allegheny Ludlum AL 304DA is tri-ply composite consisting of a dual stabilized, low carbon steel cent.. |
|||
Tensile Strength, Yield | 260 - 300 MPa | 37700 - 43500 psi | |
ArcelorMittal 260 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC260B), electroglavanized (HC260B+ZE) and Extragal®/Galvannealed (HC260BD+Z)Description: The composition and processing of these steels are designed to promot.. |
|||
Tensile Strength, Yield | 260 - 300 MPa | 37700 - 43500 psi | |
ArcelorMittal IF 260 High strength IF steel, Cold rolled Available in the following: uncoated (HC260Y), electroglavanized (HC260Y+ZE) and Extragal®/Galvannealed (HX260YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of.. |
|||
Tensile Strength, Yield | >= 260 MPa | >= 37700 psi | |
Aleris Alustar Aluminum Alloy, H321/H116; 20 - 40 mm thickness At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.Composition d.. |
|||
Tensile Strength, Yield | 260 - 470 MPa @Strain 0.200 % |
37700 - 68200 psi @Strain 0.200 % |
|
ALIMEX 7075 T651/T652 Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress-relieved by stretching a controlled amount then artificially aged. / Solution.. |
|||
Tensile Strength, Yield | 260 - 320 MPa | 37700 - 46400 psi | |
ArcelorMittal H 260 Solid solution steel, Cold rolled Available in the following: uncoated (HC260P) and electrogalvanized (HC260P+ZE) Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These ste.. |
|||
Tensile Strength, Yield | 260 - 320 MPa | 37700 - 46400 psi | |
ArcelorMittal HSLA 260 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC260LA), electroglavanized (HC260LA +ZE) and Extragal®/galfan/Galvannealed (HC260LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |
|||
Tensile Strength, Yield | 260 MPa | 37700 psi | As Cast |
AFE Technologies Cronite Standard Nickel Alloy Castings, No. HR4 High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |