Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
Multibase Multi-Pro® 2510 XGW Polypropylene Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | Rotational Molded; ASTM D882 |
NOVA Chemicals Surpass® RMs244-UG Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
PolyMirae Moplen EP300R Injection Molding Grade Polypropylene Moplen EP300R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300R is a block copolymer particularly suitable for injection.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | Rotational Molded; ASTM D882 |
NOVA Chemicals Surpass® RMs244-U Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | 5mm/min; ASTM D638 |
Mitsui TPX® MBZ230 Methylpentene Copolymer, Filled, Opaque Grade
(discontinued **) TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
Hyosung Topilene C600H PP C600H Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Very low sealSlip propertyTransparencyInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
Hyosung Topilene C600HF PP C600HF Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Low sealSlip propertyTransparencyInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
LG Chemical LUTENE-H PE0235 HDPE Description: LUTENE-H PE0235 is a materials with high toughness and rigidity suitable for cable protection It has very high resistance to stress cracking and long-term internal pressure creep proper.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
LG Chemical LUTENE-H XL1800 HDPE Description: LUTENE-H XL 1800 is a optimum materials for under-floor heating and drinking water pipe by RAM type extrusion. It is excellent product with long-term internal pressure creep property an.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
Ineos Styrenics 496N High-Impact Polystyrene Resin (NAFTA) Description: High-impact, lower flow grades for food packaging, dairy containers, lids, plates, appliance components and housings.Information provided by BASF.Ineos Styrenics purchased this product .. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | 50 mm/min; ASTM D638 |
LG Chemical SEETEC PB150 HDPE Features: This high molecular weight, hexane copolymer is tailored for high impact blow-molded containers that require:Excellent processabilityHigh impact strength at low temperatureOutstanding stre.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® SM240 Polypropylene impact copolymer Titanpro® SM240 is a high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet .. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
IRPC Polimaxx Polene GA3245 High Density Polyethylene CHARACTERISTICS: HIGH TOUGHNESS, GOOD EXTRUDABILITY, EXCELLENT IMPACT STRENGTHAPPLICATIONS: BLOW FILM EXTRUSION FOR CARRIER BAGS, GROCERY BAGS, SHOPPING BAGS, INDUSTRIAL BAGS, LINER BAGS |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
IRPC Polimaxx Polene GG3245 High Density Polyethylene CHARACTERISTICS: EXCELLENT ENVIRONMENTAL STRESS CRACKING RESISTANCE (ESCR) EXCELLENT IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH TOUGHNESSAPPLICATIONS: BLOW MOLDING/ SHEET/ THERMOFORMING EXTRUSION CO.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ H2001WC High Density Polyethylene Wire & Cable Grade Key Characteristics:Excellent environmental stress cracking resistance (ESCR), high mechanical properties, high speed extrusionRecommended Applications:Jacketing of fiber optical cablesJacketing of .. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ H6105JU High Density Polyethylene Injection Molding Key Characteristics:Good processabilityWide service temperatureHigh rigidityGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drinks, bottles, pallet, garbage bins, .. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | at 100% elongation; ASTM D412 |
Lubrizol Estane® S364D Thermoplastic Polyurethane Type: Estane® S364D is a Shore 65D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | at 300% elongation; ASTM D412 |
Lubrizol Estane® X-595A-11 Thermoplastic Polyurethane Type: Estane® X-595A-11 is a Shore 97A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Extrusion.Available in AsiaInformation Provided by The Lubr.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | |
Zylog Hipolyene® 3020 HC RM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | |
Zylog Hipolyene® 8025 HC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
Eastman Tenite 285A2R30018 Cellulose Acetate Butyrate, Natural, Trsp Applications:OphthalmicsOptical safety framesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, cla.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
Eastman Tenite 285A3R30018 Butyrate Natural, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength, Yield | 23.5 MPa | 3410 psi | ASTM D638 |
Entec Hypro™ PPH-CC40 Natural Homopolymer Polypropylene, 40% Calcium Carbonate Filled Information provided by Entec |