Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.2 MPa | 2350 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W3201 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon® W3201 is UL recognized for UL 94 V0 per QMFZ2, and is suitable for injection molding. This product meets UL 105°C, AWM, and Mil-W-76 80°C insulation.NOTE: Typical Properties of Molded Slab .. |
|||
Tensile Strength, Yield | 16.2 - 16.7 MPa | 2350 - 2420 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Tensile Strength, Yield | 16.2 - 16.7 MPa | 2350 - 2420 psi | ASTM D1708 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G70G Green Perfluoroelastomer Excellent chemical resistance, steam resistance and good mechanical properties. Color coded for identification.Applications: Specially developed for critical applications where good chemical resista.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D412 |
Teknor Apex APEX® 3201-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D412 |
Teknor Apex APEX® 3301-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D412 |
Teknor Apex APEX® 94-A0098A-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D412 |
Teknor Apex Flexalloy® 3501-65-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D638; ISO 527-2 |
Styron INSPIREâ„¢ TF1301 Thermoplastic Polyolefin Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SFW 5500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Uses: Footwear; General Purpose Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SGH 5500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Uses: Garden Hose Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | 20 in/min; ASTM D638 |
Teknor Apex Sinvicomp SMG 5500 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Food Contact Acceptable; Non-Toxic Uses: Toys Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D412 |
Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D412 |
Borealis Visico™ LE4423/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | At 20 in/min; ASTM D638 |
Borealis Visico™ ME4425/LE4462 Scorch Retardant Silane Crosslinkable MDPE Track Resistant Cable Insulation Visico ME4425/LE4462 is a combination of LE4425, a Medium Density Visico base resin and a masterbatch, LE4462, which contains catalyst, carbon black, UV stabilizers and antioxidants. The LE4462 mas.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D638 |
Washington Penn Medium Impact Copolymer 40% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D412 |
Borealis Visico™ LE4421/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4421/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D-638 |
Axiall 835WA Wire & Cable Flexible PVC AWM for SPT, SJT and SVT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D-638 |
Axiall 9175 Wire & Cable Flexible PVC Oil resistant tray cable jacket. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D-638 |
Axiall 12860 Wire & Cable Flexible PVC 80C liquid tight conduit.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D-638 |
Axiall 8750 Moldings & Extrusions Flexible PVC A clear, high quality extrusion and molding compound formulated to give good low temperature properties and good heat stability.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpora.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D-638 |
Axiall 8751 Moldings & Extrusions Flexible PVC Clear, UV stabilized extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D-638 |
Axiall 12862 Wire & Cable Flexible PVC Non-lead 80C liquid tight conduit compound according to UL360.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D412 |
Borealis Visico™ LE4423/LE4460/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4460/LE4432 is a black, halogen-based flame retardant, moisture-induced crosslinking polyethylene compound that is designed for use as low wire insulation and jacketing. The combina.. |
|||
Tensile Strength, Yield | 16.2 MPa | 2350 psi | ASTM D-638 |
Axiall 14811 Wire & Cable Flexible PVC Matte finish general purpose jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |