Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 159 MPa | 23100 psi | 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ SF-30CF/15T Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 159 MPa | 23100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP 9X98026 PA 46 (Europe-Africa-Middle East) LNP* Lubricomp* 9X98026 is a compound based on PA4.6 resin containing Barium Sulfate, PTFE and Carbon Fiber |
|||
Tensile Strength, Yield | 159 MPa | 23100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66 LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for .. |
|||
Tensile Strength, Yield | 159 MPa | 23100 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ASTM A 424 Type III, I-F Enamel Enameling Carbon Steel I-F Enameling Steel is a vacuum degassed, titanium stabilized steel. I-F Enameling Steel can be used for ground coat and two coat-one fire porcelain enameling systems. It is not recommended for us.. |
|||
Tensile Strength, Yield | 159 MPa | 23100 psi | |
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel (EDDS), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Tensile Strength, Yield | 159 MPa | 23100 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F®) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Tensile Strength, Yield | 159 MPa | 23100 psi | ASTM D638 |
Ashley Polymers Ashlene® 830L-25G Nylon 6, 25% Glass Reinforced A 25% glass fiber reinforced Nylon 6 designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 type material.Data pr.. |