Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Precision Polymer Engineering E70I Ethylene Propylene Rubber Resin cured Ethylene Propylene Terpolymer, 70-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated for applications involving water and steam.Applications: Recommended for us.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Precision Polymer Engineering N60W Nitrile Rubber White Nitrile Butadiene Rubber (NBR), 55-65 °IRHD. Copolymer of acrylonitrile and butadiene. Formulated using only those ingredients determined by the United States Food and Drug Administration (F.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Precision Polymer Engineering N70M Nitrile Rubber Nitrile Butadiene Rubber (NBR), 68-78 °IRHD. Copolymer of acrylonitrile and butadiene. To meet BS2751 BA70 and ASTM D2000/SAE J200 line call-out 2MBG 714, B14, EA14, EF11, EF21, EO14, EO34, F17.Ap.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G60H Perfluoroelastomer Special, pure white compound with excellent high temperature properties and wide chemical resistance. Extremely low outgassing properties.Applications: For use in applications which require exposur.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Precision Polymer Engineering V71C Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Terpolymer of vinylidene difluoride and hexafluoropropylene tetrafluoroethylene. Compounded to have extremely low temperature capability, Glass transition tem.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Precision Polymer Engineering V75A Fluoroelastomer Compound Signal Blue, Fluoroelastomer Rubber, 70 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Diesel liner ring grade.Applications: Excellent resistance to oils, fuels and hydraulic flu.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
NOVA Chemicals Novapol® PI-3526-A LLDPE Masterbatch Resin
(discontinued **) Molded Plaque Properties. Features: high flow.Applications: general purpose, housewares.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 13.0 - 65.0 MPa | 1890 - 9430 psi | Average value: 41.4 MPa Grade Count:92 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
LyondellBasell Lupolen® 3010 K LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
LyondellBasell Lupolen® 3020 F LDPE Blown film, injection moldings, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
LyondellBasell Lupolen® 3020 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
LyondellBasell Lupolen® 3040 D LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Strength, Yield | >= 13.0 MPa | >= 1890 psi | |
Kazanorgsintez 297-285 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MH0500A PP (Asia Pacific) LNP THERMOCOMP* MH0500A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP) LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s). |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D412 |
Teknor Apex APEX® 94-A0098A-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIM 5039 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Strength Uses: Electrical/Electronic Applications < Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
Trelleborg B747 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | |
Trelleborg B939 Nitrile Rubber Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Trelleborg Horda Cable E8400 Easy Strippable Semiconductive Shielding E8400 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8400 meets the requirements as be.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Trelleborg Horda Cable E8561 Strippable Semiconductive Shielding E8561 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8561 meets the requirements as bel.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Eastman Eastman AP007 Copolyester Applications:Automotive componentsBreathable filmsElectronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsOffice furniturePackagingPolymer modificationProfilesRubber an.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | 2 in/min, Type IV bar; ASTM D-638 |
Chevron Phillips Marlex® HHM TR-232 Polyethylene; Enhanced Low density linear polyethylene. This low density, linear resin is tailored for blow molded containers that require: Excellent processabilityExcellent ESCRApplications: Typical blow molded applica.. |
|||
Tensile Strength, Yield | 13.0 MPa @Strain 300 % |
1890 psi @Strain 300 % |
ASTM D412 |
Dow Buna® SB 1721 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Buna® SB 1721 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. It is plasticized with 37.5 parts of an aromatic oil in relation to solid rubber. A disc.. |
|||
Tensile Strength, Yield | 13.0 MPa @Strain 300 % |
1890 psi @Strain 300 % |
ASTM D412 |
Dow Buna® SB 1723 Cold polymerized Emulsion Styrene Butadiene Rubber (E-SBR) Buna® SB 1723 - Schkopau is manufactured by cold polymerization using mixed rosin acid / fatty acid soaps. It is plasticized with 37.5 parts of a TDAE oil in relation to solid rubber. A discolori.. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ISO R 527 |
Addiplast Addilene J 380 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ISO 527 |
A.D. Compound Adene NCZAG Copolymer 70% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Tensile Strength, Yield | 13.0 MPa | 1890 psi | ASTM D638 |
Huntsman PE2067 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: High flow resin, provides excellent gloss and surface characteristics, and minimum cycle time.Applications: Injection molding: lids.FDA Notes: Conforms to FDA.. |