Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 81520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Tensile Strength, Yield | 96.5 - 110 MPa | 14000 - 16000 psi | Average value: 105 MPa Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Tensile Strength, Yield | 96.55 MPa | 14000 psi | ASTM D638 |
Lucent Polymers G6-15 Nylon 6, 15% Glass Fiber Reinforced Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 96.55 MPa | 14000 psi | ASTM D638 |
Lucent Polymers GPC-0202 20 Polycarbonate, Glass Reinforced, Injection Grade Recycled ContentAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 GF13 SS10 BK 13/10% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Stainless Steel Reinforcement, 13/10% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® ABS GF30 A1 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF/B20 A3 BK 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: .. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Star Plastics PCGF20 Molding Grade PC with 20% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® PEEK 150 Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® PEEK 450 BK Availability: North AmericaForms: PelletsFeatures: High ViscosityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® POM CO GF/M30 UV BK 30% Glass Milled/Glass Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Milled/Glass Fiber, 30% Filler by WeightAdditive: UV StabilizerFeatures: Copolymer and Chemically CoupledAppearance: BlackInforma.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/ABS 1120 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 GF13 FR-N BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® TPX-HTN-03002 A 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightFeatures: Platable and High Temperature StrengthUL File Number: E157318Information provided by TP C.. |
|||
Tensile Strength, Yield | 96.5 MPa @Temperature 22.8 °C |
14000 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Clariant Renol PA211G13 Nylon 6, 13% Glass Fiber Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Clariant Renol PCSP0009 Polycarbonate, 15% Glass Fiber, Silicone Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-40FG-0874 40% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Asahi Kasei Thermylene® P7-30FG-0684 30% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Asahi Kasei Thermylene® P7-30FG-0874 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 96.4 MPa | 14000 psi | ASTM D638 |
Ashley Polymers Ashlene® 61M Nylon 66, 40% Mineral reinforced A 40% mineral reinforced general purpose Nylon 66 resin with superior stiffness and dimensional stability.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 GF15 FR-N 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized, Halog.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® PVDF CF10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |