Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 950 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
Typical, Longitudinal Direction |
Industeel CLC 1.2316 Prehardened (300HB) and Corrosion Resistant Mold Steel Description: CLC 1.2316 is a 16%Cr 1% Mo with improved corrosion resistance properties, thanks to the chromium/molybdenum additions. The high cleanliness/homogeneity of the steel makes it specially .. |
|||
Tensile Strength, Yield | 950 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
Typical, Longitudinal Direction |
Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are c.. |
|||
Tensile Strength, Yield | 950 MPa @Strain 0.200 %, Temperature 95.0 °C |
138000 psi @Strain 0.200 %, Temperature 203 °F |
|
Haynes 242® alloy, cold rolled sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 950 MPa @Strain 0.200 %, Temperature 550 °C |
138000 psi @Strain 0.200 %, Temperature 1020 °F |
Precipitation Hardened prior to test |
Special Metals INCOLOY® Alloy 909 A nickel-iron-cobalt alloy with a silicon addition and containing niobium and titanium for precipitation hardening. It is similar to INCOLOY alloys 903 and 907 in that it has low thermal expansion .. |
|||
Tensile Strength, Yield | 950 - 1250 MPa @Strain 0.200 % |
138000 - 181000 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 1200 DP High-strength Steel The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel .. |
|||
Tensile Strength, Yield | 950 MPa | 138000 psi | |
SSAB Tunnplat Domex® 014 BOR Oil quenched Boron Steel Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron .. |
|||
Tensile Strength, Yield | 950 MPa | 138000 psi | |
ThyssenKrupp SECURE 400 Structural Steel This Material Specification applies to the alloyed, liquid-quenched and tempered high-strength special steel SECURE 400 for civil use, this is usually produced in thickness from 3 mm up to 50 mm.App.. |
|||
Tensile Strength, Yield | 950 MPa | 138000 psi | 0° |
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, High Strength 6k carbon Balanced fabric 285 g/m2 Information provided by HexCel |
|||
Tensile Strength, Yield | >= 950 MPa @Strain 0.200 % |
>= 138000 psi @Strain 0.200 % |
|
CLAL-MSX NICLAFOR® 1000 THX Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Tensile Strength, Yield | 951 MPa | 138000 psi | Hardened 1900°F, Tempered 1000°F |
ATI Allegheny Ludlum 420 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 952 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 482°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Tensile Strength, Yield | 950 - 1200 MPa | 138000 - 174000 psi | |
ArcelorMittal MartINsite® 1200 Cold Rolled Steel Description: The family of MartINsite steels extends ArcelorMittal's range of Ultra High Strength Steels (UHSS). These steels allow the realization of lightweight structural elements by a forming me.. |
|||
Tensile Strength, Yield | 951 MPa @Strain 0.200 %, Temperature 316 °C |
138000 psi @Strain 0.200 %, Temperature 601 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | 951 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 538°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Tensile Strength, Yield | 952 MPa @Strain 0.200 % |
138000 psi @Strain 0.200 % |
|
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 746°C (1375°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |