Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 828 MPa | >= 120000 psi | 0.2% proof |
Kobe Steel KS EL-F Alpha-Beta Titanium Alloy, Annealed Nominal Composition: Ti-4.5 Al-4 Cr-0.5 Fe-0.2 C Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excellent balance b.. |
|||
Tensile Strength, Yield | >= 827 MPa | >= 120000 psi | 0.2% proof |
Kobe Steel KS6-2-4-2 Alpha Titanium Alloy, AMS 4976, Solution treated and aged Nominal Composition: Ti-6 Al-2 Sn-4 Zr-2 Mo Applications: Jet engine parts, engine valves.Features:Heat resistant. Information provided by Kobe Steel |
|||
Tensile Strength, Yield | >= 828 MPa | >= 120000 psi | 0.2% proof |
Kobe Steel KSTI-9 Alpha-Beta Titanium Alloy, ASTM Gr. 35, Annealed (coil, sheets) Nominal Composition: Ti-4.5 Al-2 Mo-1.6 V-0.5 Fe-0.3 Si-0.03 C Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excel.. |
|||
Tensile Strength, Yield | 827 - 1030 MPa @Strain 0.200 % |
120000 - 150000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 827 - 1030 MPa @Strain 0.200 % |
120000 - 150000 psi @Strain 0.200 % |
|
Materion BrushCAST® 21C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | >= 827 MPa @Strain 0.200 % |
>= 120000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 AT120 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Yield | >= 827 MPa @Strain 0.200 % |
>= 120000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 AT120 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Yield | >= 830 MPa | >= 120000 psi | |
MetalTek RENE® 220 Centri-Vac Nickel Cobalt Based Alloy Information provided by MetalTekWrought Grade RENE® 220 |
|||
Tensile Strength, Yield | 825 MPa @Strain 0.200 %, Temperature 650 °C |
120000 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 25 alloy, cold worked sheet, 20 % cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 827 MPa | 120000 psi | Up to 1.5 inches; Un-Nitrided |
Latrobe LSSâ„¢ 135M Nitriding Steel (ASTM A355 Class A) TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured fr.. |
|||
Tensile Strength, Yield | >= 827 MPa | >= 120000 psi | |
Materion Alloy M65 (C17465) Beryllium Copper Rod Alloy M65 (C17465) is a machinable, high-performance, copper beryllium rod alloy from Brush Wellman. M65 has excellent strength, conductivity, and resistance to elevated temperature stress relaxatio.. |
|||
Tensile Strength, Yield | 827 - 1069 MPa | 120000 - 155000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH4, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | 827 - 1030 MPa @Strain 0.200 % |
120000 - 150000 psi @Strain 0.200 % |
|
Materion BrushCAST® 20CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Yield | 826 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
Typical, Transverse Direction |
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections Description: CLC 1.2738 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, Nickel carbon and manganese additions are optimized to have a fully .. |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Universal Wire Works 6Al-4V (AMS 4954) Titanium Alloy Filler Metal Universal 6Al-4V titanium alloy is often repaired with the gas tungsten arc or gas metal arc welding process, provided adequate inert gas shielding of the filler wire and deposited weld metal is pro.. |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Universal Wire Works 6Al-4V (ELI) (AMS 4956) Titanium Alloy Filler Metal Universal titanium alloy 6Al-4V (ELI) is similar to type 6Al-4V in chemical analysis with the exception of Extra Low Interstitial gases (ELI). By controlling these contaminating gases the fracture t.. |
|||
Tensile Strength, Yield | >= 830 MPa | >= 120000 psi | 50<x=60mm |
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength, Yield | >= 830 MPa | >= 120000 psi | 60<x=80mm |
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength, Yield | >= 830 MPa | >= 120000 psi | 80<x=100mm |
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Tensile Strength, Yield | >= 828 MPa @Strain 0.200 % |
>= 120000 psi @Strain 0.200 % |
Longitudinal |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
Tensile Strength, Yield | >= 828 MPa @Strain 0.200 % |
>= 120000 psi @Strain 0.200 % |
L and LT Directions |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265 Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265; other specific form/thickness entries a.. |
|||
Tensile Strength, Yield | 830 MPa @Temperature 80.0 °C |
120000 psi @Temperature 176 °F |
Tensile Warp, Wet; Pr EN 2597 B |
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System HexFlow® RTM 6 is a monocomponent resin already degassed, specifically developed to fulfill the requirements of the aerospace and space industries in advanced resin transfer moulding (RTM) process... |
|||
Tensile Strength, Yield | 827 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, 48% Cold Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Vacuum arc remelted (VAR), low carbon version of Type 316 stainless. The secondary premium melting step (VAR) imparts impro.. |
|||
Tensile Strength, Yield | 830 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
Carpenter Pyromet® CTX-3 Superalloy, Heat Treated Data provided by Carpenter Technology Corporation.Pyromet® alloy CTX-3 is a high strength, precipitation hardenable superalloy which exhibits a low CTE over a broad temperature range. This alloy a.. |
|||
Tensile Strength, Yield | 827 - 930 MPa @Strain 0.200 % |
120000 - 135000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TS02 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 828 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 5 Titanium 6Al-4V (UNS R56400) Uses: blades, discs, rings, airframe, fasteners, components, vessels, cases, hubs, forgings.Mechanical property data below is typical of annealed samples at room temperature.Information provided by .. |
|||
Tensile Strength, Yield | 828 MPa @Strain 0.200 % |
120000 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 422 Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal Data provided by Allvac.Applications: Jet engine parts, brackets, disks, bolts, blades fasteners, aircraft components. Parts for steam and gas turbines, engines. |
|||
Tensile Strength, Yield | 824 MPa | 120000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 30% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |