Ametek AM 388™ Alloy (UNS C72650) TS02

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Ametek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ametek AM 388™ Alloy (UNS C72650) TS02.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and switches.Benefits include combination of high strength and formability, high conductivity, available in mill hardened or age hardenable tempers, no distortion during aging, no fixturing required, excellent solderability and resistance to stress relaxation during high temperature (over 400°F, 200°C) soldering, fine grain size, excellent corrosion resistance bare and easy to plate when required, low initial cost, and additional savings during processing.Spinodal Age Hardening Treatment 725°F (385°C)/2 hrs.
Physical Properties Metric English Comments
Density 8.87 g/cc
0.320 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 300 - 360
300 - 360
Tensile Strength, Ultimate 930 - 999 MPa
135000 - 145000 psi
Tensile Strength, Yield 827 - 930 MPa

@Strain 0.200 %
120000 - 135000 psi

@Strain 0.200 %
Elongation at Break 6.0 - 9.0 %
6.0 - 9.0 %
typical
Modulus of Elasticity 124 GPa
18000 ksi
Component Elements Properties Metric English Comments
Copper, Cu 87 %
87 %
as balance
Nickel, Ni 7.0 - 8.0 %
7.0 - 8.0 %
Other <= 0.50 %
<= 0.50 %
Tin, Sn 4.5 - 5.5 %
4.5 - 5.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000115 - 0.0000123 ohm-cm
0.0000115 - 0.0000123 ohm-cm
Conductivity 14 - 15% IACS