Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 724 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
FloMet 17-4 PH Stainless Steel, As Sintered FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Yield | >= 725 MPa | >= 105000 psi | |
MetalTek GTD 222® Centri-Vac Nickel Cobalt Based Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | 724 MPa | 105000 psi | Tempered at 1150°F, 4hr |
Latrobe Lescalloy® 15-5 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 15-5 VAC-ARC steel is a precipitation hardening martensitic stainless steel commonly considered to be a compositional modification of 17-4 with minimal delta ferrite. A wide range of mec.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 %, Thickness <=0.400 mm |
>= 105000 psi @Strain 0.200 %, Thickness <=0.0157 in |
CWSR, 0.016 in. Wall & Below; AMS 4944/4945 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 %, Thickness >=0.400 mm |
>= 105000 psi @Strain 0.200 %, Thickness >=0.0157 in |
CWSR, Above 0.016 in. Wall; AMS 4944/4945 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Yield | 725 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
Haynes 25 alloy, cold worked sheet, 10% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 % |
>= 105000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 2 Cold Worked Cold Worked applies to tensile values and are for 0.25 to 4 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resis.. |
|||
Tensile Strength, Yield | 725 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
Precipitation Hardened. Value at room temperature |
Special Metals NIMONIC® Alloy 90 A precipitation-hardenable nickel-chromium-cobalt alloy having high stress-rupture strength and creep resistance at temperatures to about 1700°F (920°C). The alloy also has good resistance to.. |
|||
Tensile Strength, Yield | 724 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
Schmolz + Bickenbach MoldMAX® V Copper Alloy Description: Brush Wellman’s MoldMAX® V (MMV) is a high conductivity, moderately high strength, copper nickel silicon chromium alloy. Applications include injection mold and blow mold cores .. |
|||
Tensile Strength, Yield | >= 725 MPa @Strain 0.200 % |
>= 105000 psi @Strain 0.200 % |
|
Schmolz + Bickenbach UGICHROM 4542 Martensitic Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength, Yield | >= 724 MPa | >= 105000 psi | |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and w.. |
|||
Tensile Strength, Yield | 724 - 800 MPa | 105000 - 116000 psi | 0.2% offset |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Yield | 724 MPa | 105000 psi | Proportional Limit |
ECOMold 95 Copper Mold Material ECOMold® copper alloys (beryllium-free) are designed specifically for plastics industry applications. ECOMold® 95 has a superior combination of thermal conductivity, hardness, and tensile strengt.. |
|||
Tensile Strength, Yield | 724 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
Tension |
Crucible Steel Aquamet® 17 Martensitic Steel AQUAMET 17 is a precipitation-hardening, martensitic stainless steel. Because it is hardened by a heat treatment, it provides high strength regardless of the diameter. It also offers good toughness .. |
|||
Tensile Strength, Yield | 723 MPa | 105000 psi | |
CMW® THERMKON® 62 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | 724 MPa | 105000 psi | Hard |
California Fine Wire Nickel A 200 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 724 MPa @Strain 0.200 %, Temperature -253 °C |
105000 psi @Strain 0.200 %, Temperature -423 °F |
Longitudinal |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Tensile Strength, Yield | 723 - 861 MPa | 105000 - 125000 psi | |
Ametek AM 388™ Alloy (UNS C72650) TM06 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 727 MPa | 105000 psi | Hardened 1900°F, Tempered 1200°F |
ATI Allegheny Ludlum 440A Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 721 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 43.6% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Tensile Strength, Yield | 725 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 418™ Special (Greek Ascoloy) Martensitic Stainless Steel Uses include engine braces, turbine exhaust components, exhaust struts, stiffeners, and ducts.Information provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | 727 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
Tensile Strength, Yield | <= 725 MPa @Strain 0.200 % |
<= 105000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated Plate, UNS N07718 Allegheny Ludlum Altemp 718 alloy is an austenitic nickel-base superalloy which is used in applications requiring high strength to approximately 760 degrees Celsius and oxidation resistance to appro.. |
|||
Tensile Strength, Yield | 725 MPa @Strain 0.200 %, Temperature 95.0 °C |
105000 psi @Strain 0.200 %, Temperature 203 °F |
|
Haynes 242® alloy, hot rolled plate, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good thermal.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 % |
>= 105000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 2 Cold Worked Level 2 Cold Worked applies to tensile and hardness properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic all.. |
|||
Tensile Strength, Yield | 725 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
Kennametal Stellite Stellite® 31 PM after P/M processing, aged 8 hours at 802°C air cooled Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we.. |
|||
Tensile Strength, Yield | >= 724 MPa @Strain 0.200 % |
>= 105000 psi @Strain 0.200 % |
|
Materion ToughMet® T3 CX105 (OD ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have engin.. |
|||
Tensile Strength, Yield | 724 MPa @Strain 0.200 % |
105000 psi @Strain 0.200 % |
|
Schmolz + Bickenbach MoldMAX XL® Copper Alloy Description: Brush Wellman’s MoldMAX XL® is a high strength copper mold alloy with good thermal conductivity. The alloy contains no beryllium and is available in sections as large as 12” thick. .. |