Polymer Property : Tensile Strength, Yield = 70.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.3 MPa
10200 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ PPH-40G Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
PTS Trilac® ABS-GF3000-BK 30% Fiberglass Black ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 70.3 MPa
10200 psi
Clear Casting
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin
TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA..
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
LG Chemical Lupox® PBT-GP-2306FA 30% GFR Flame Retardant, UV Stabilized PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
Techmer ES Electrablend® PC SS10 10% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: ConductiveInformation provided by TP Composites, Inc.
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
Techmer ES Statiblend® PC FR BK
Availability: North AmericaForms: PelletsAntistaticFeatures: Flame Retardant and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc.
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
PlastxWorld Veroplas PB2002 Nylon 66
impact modified, unfilled injection molding gradeInformation provided by PlastxWorld Inc.
Tensile Strength, Yield 70.3 MPa
10200 psi
Clear Casting
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin
TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA..
Tensile Strength, Yield 70.3 MPa

@Thickness 3.18 mm
10200 psi

@Thickness 0.125 in
6 mm/min; ASTM D638
Chi Mei Acryrex® CM-205 PMMA
High heat injection grade. It can resist high temperature. High mechanical strength.Applications: The indicator cover of scooter and automobile/sun glasses/digital watch cover.Features:Good Weather ..
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black
Data provided by Clariant Masterbatches
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
Clariant BRU2000 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black
Data provided by Clariant Masterbatches
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant
Data provided by Clariant Masterbatches
Tensile Strength, Yield 70.3 MPa
10200 psi
ASTM D638
Asahi Kasei Thermylene® P6-30FM-0378 30% Glass/Mineral Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Tensile Strength, Yield 70.3 MPa
10200 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
PolyOne Edgetek® PF-1000 Polysulfone  (discontinued **)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..