Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 6.89 MPa | 999 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-PB-069-BMX Natural Polyether Block Amide (PEBA-Ether) Information provided by PolyOne |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 6.89 - 13.8 MPa | 1000 - 2000 psi | ASTM D1708 |
Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
Tensile Strength, Yield | 6.89 MPa | 999 psi | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 45H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce.. |
|||
Tensile Strength, Yield | >= 6.89 MPa @Strain 300 % |
>= 1000 psi @Strain 300 % |
|
Sibur SKD 1st Grade Butadiene Rubber (BR) BR 1220. It is used in tires and the rubber and asbestos technical industries. Rubbers produced on a base of butadiene rubber are extremely resistant to wearing. |
|||
Tensile Strength, Yield | >= 6.89 MPa @Strain 300 % |
>= 1000 psi @Strain 300 % |
|
Sibur SKD Superior Quality Butadiene Rubber (BR) BR 1220. It is used in tires and the rubber and asbestos technical industries. Rubbers produced on a base of butadiene rubber are extremely resistant to wearing. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412-97 |
Saint-Gobain Norprene® A-60-F Food Process Tubing Formulation Description: Norprene® Food Process Tubing, Formulation A-60-F: Formulated to withstand the high temperatures frequently occurring during food and beverage processing, Norprene® Food Process.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412-98 |
Saint-Gobain Norprene® A-60-G Industrial Grade Tubing Formulation Description: Norprene® Industrial Grade Tubing, Formulation A-60-G: Norprene® Industrial Grade Tubing outperforms neoprene, EPDM and other general-purpose tubings in test after test and appl.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex APEX® 3210-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3302-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex APEX® 3310-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2750 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2760 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2785H Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2840E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 2890M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | |
Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete a.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 302 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF302 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | >= 6.89 MPa | >= 1000 psi | ASTM D638 |
Buckeye Polymers BP FLEX D4107 C BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3201-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 38-096 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerOpaqueApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDisclai.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | TM R050-36 |
Resinlab® SEC1222 Silver Filled Epoxy Adhesive Resinlab™ SEC1222 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1222 provides excellent electrical conductivit.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 37-033 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A therm.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 584 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerOpaqueApplications:Multi-PurposeFDA (Food Contact)Processing Method:Injection MoldingPolyOne First ChoiceDisclaimer: A thermoplastic elas.. |
|||
Tensile Strength, Yield | 6.89 MPa | 1000 psi | TM R050-36 |
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi.. |