Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 52.4 MPa | 7600 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Oxford Polymers 802-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec.. |
|||
Tensile Strength, Yield | 52.4 - 79.3 MPa | 7600 - 11500 psi | Average value: 63.6 MPa Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM Data |
Americas Styrenics Styron® 663 Polystyrene
(discontinued **) STYRON® 663 general purpose polystyrene resin is an additive free resin with excellent strength, clarity, and high heat resistance. When used unmodified for the manufacture of food contact articles.. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM Data |
Americas Styrenics Styron® 685 Polystyrene
(discontinued **) STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use.. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM Data |
Americas Styrenics Styron® 685P Polystyrene
(discontinued **) STYRON® 685P general purpose polystyrene resin is a high heat resin with good strength, moldability/processability, and excellent clarity. This resin is typically used in consumer electronic applic.. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
I. Stern WC-103 General Purpose Crystal Polystyrene Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. Inc. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Global GP-110 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® NY2115 Nylon 66 Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 52.4 MPa @Temperature 23.0 °C |
7600 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Polene GP110 Polystyrene APPLICATIONS: EXTRUSION SHEET, HOUSEHOLD PRODUCTS VACUUM SHEET , FOOD PACKAGING, TOY, SANITARY WARE, etc. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Techmer ES HiFill® ABS E GM5 LE 5% Glass Filled Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Spartech Acrylloy 7 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Spartech Acrylloy F Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Spartech Tuf-Glas Impact Modified Acrylic Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Techmer ES HiFill® TPU GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Techmer ES Plastiblend® PC/PBT IM 5220 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D 638 |
Styrolution PS 1200/1201 GPPS Extrusion / thermoforming foam sheetHigh melt strengthHigh StiffnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D 638 |
Styrolution PS 1290/1291 GPPS Extrusion / thermoforming foam sheetLow residual styrene monomer contentHigh melt strength and stiffnessUL Classification 94 HB for 1290Information provided by Styrolution |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Techmer ES HiFill® PP GF/M35 CC BK 35% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Techmer ES Luriblend® PSU TL20 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM 638 |
PlastxWorld CEVIAN® LMB10 Laser Markable Grade ABS Black MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Total PSC 585 Polystyrene Polystyrene 585 is a high molecular weight, low melt flow, crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. 585 also mak.. |
|||
Tensile Strength, Yield | 52.4 MPa | 7600 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-10FG-0600 10% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |