Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
PolyMirae Moplen HF524J BDDP Film Grade Polypropylene
Moplen HF524J is the Addiform polypropylene. Compared to ordinary pelletized polypropylene, Addiform gives significant advantages in terms of improved productivity, better processing and lower energ..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
PolyMirae Moplen HF550K Stretch/Yarn, Monofilament Grade Polypropylene
Moplen HF550K is the ADDIFORM polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Its appearance is spherical, white particle with diameter of 1mm ..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
PolyMirae Moplen HP525J BDDP Film Grade Polypropylene
Moplen HP525J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP525J is a homopolymer particularly suitable for Metallizable BOPP..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
PolyMirae Moplen HP557G Stretch Grade Polypropylene
Moplen HP557G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP557G is a homopolymer suitable for high strength rope, container ..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
PolyMirae Moplen HP600R Injection Grade Polypropylene
Moplen HP600R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP600R is a homopolymer typically used in injection molding of food..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene
Moplen HP740T is a nucleated polypropylene HOMO polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP740T is a homopolymer selected by customers for use in t..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
PolyMirae Moplen HP425J BDDP Film Grade Polypropylene
Moplen HP425J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. MIRAEPOL T28C is a homopolymer particularly suitable for BOPP (Tender) fil..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
PolyMirae Moplen HP450J Stretch/Yarn, Monofilament Grade Polypropylene
Moplen HP450J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP450J is a homopolymer typically used by customers in Raffia and Y..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene
Moplen HP500G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP500G is a homopolymer particularly suitable for sheet, thermofor..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Hyosung Topilene F600 PP
F600 Film Grade HomopolymerApplications: IPPCharacteristics:ProcessabilityTransparencyInformation provided by Hyosung Corporation
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Hyosung Topilene F603 PP
F603 Film Grade HomopolymerApplications: CPPCharacteristics:ProcessabilityTransparencystiffnessInformation provided by Hyosung Corporation
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Hyosung Topilene J700 PP
J700 Injection General HomopolymerApplications: General injectionCharacteristics:ProcessabilityStiffnessInformation provided by Hyosung Corporation
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Hyosung Topilene S700 PP
S700 Fiber Grade HomopolymerApplications:Continuous filamentBCFCharacteristics:ProcessabilityInformation provided by Hyosung Corporation
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Hyosung Topilene S800 PP
S800 Injection Special Purpose GradeApplications:Electric home applianceHousewares applianceCharacteristics:Heat resistanceInformation provided by Hyosung Corporation
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Hyosung Topilene S800F PP
S800F Fiber Grade HomopolymerApplications:Staple fiberBCFFine denier filamentCharacteristics:ProcessabilityInformation provided by Hyosung Corporation
Tensile Strength, Yield 36.3 MPa

@Thickness 3.20 mm
5260 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical ALPHALAC SG960 HIPS
Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical
Tensile Strength, Yield 36.3 MPa

@Thickness 3.20 mm
5260 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOL GP3200 PP+MF20%
Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Tensile Strength, Yield 36.3 MPa
5260 psi
50 mm/min; ASTM D638
LG Chemical MI-770 MIPS
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
IRPC Polimaxx Polene 111JX TA8 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 40% TALCUM REINFORCED HIGH STIFFNESSAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Hyosung Topilene J800 PP
J800 Injection General HomopolymerApplications: General injectionCharacteristics:FlowabilityStiffnessInformation provided by Hyosung Corporation
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Hyosung Topilene J800R PP
J800R Injection Special Purpose GradeApplications:Electric home applianceHousewares applianceCharacteristics:Long-term heat resistanceInformation provided by Hyosung Corporation
Tensile Strength, Yield 36.3 MPa

@Thickness 3.20 mm
5260 psi

@Thickness 0.126 in
50 mm/min; ASTM D638
LG Chemical AF360 ABS, TBBA-free Flame Retardant
Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b..
Tensile Strength, Yield 36.3 MPa
5260 psi
50 mm/min; ASTM D638
LG Chemical SG-950 Alphalac Polystyrene
High strength, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electr..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
IRPC Polimaxx Polene 1111NX TA4 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER WITH 20% TALCUM REINFORCEDAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES
Tensile Strength, Yield 36.3 MPa
5260 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 36.3 MPa
5260 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
SCG Chemicals EL-Leneâ„¢ H6240B High Density Polyethylene Blow Molding
Key Characteristics:Good stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthGood appearanceOdorlessSafe for food contactGood printabilityRecommended App..
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
SCG Chemicals EL-Leneâ„¢ H6430BM High Density Polyethylene Blow Molding
Key Characteristics:Excellent stiffnessGood processabilityOdorlessSafe for food contactGood printabilityRecommended Applications:Bottles for drinking water, fruit juice, soft drink, milkAutomotive p..