Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH020 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applications. Applications: Bags & Pouches; Raffia/Tapes/Strapping; Peelable.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film COPYLENE™ CH020-02 is a polypropylene homopolymer resin suitable for thermoforming, sheet and film fiber applications. Applications: Opaque Containers. Equivalent to Pro-fax® HL783HInformation pro.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CH020-03 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020-03 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applicationsApplications: Bags & Pouches, Raffia/Tapes/Strapping, Peelabl.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH034 Polypropylene, Homopolymer, BOPP COPYLENE™ CH034, a polypropylene homopolymer resin, is designed for the production of biaxially oriented polypropylene films (BOPP). Potential uses include metalized film applications, (either dire.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 27% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Global TPP-120 20% Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Ineos N00N-00 Polypropylene Impact Copolymer Grade N00N-00 is a fractional melt flow rate, high impact copolymer polypropylene specifically designed for non-pressure structured wall pipe but can also be used in other extrusion applications req.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PP1-2000RX Biocompatible Polypropylene Homopolymer A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PP1-2001A Antimicrobial Polypropylene Homopolymer A 20 melt injection molding grade of Polypropylene homopolymer containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information pro.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PP1-2002AF Food Grade Polypropylene Homopolymer A 20 melt injection molding grade of Polypropylene homopolymer with FDA food contact approval and antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PP1-2005ARX Biocompatible Polypropylene Homopolymer A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All in.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Ineos N01N-00 Polypropylene Impact Copolymer Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properti.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Spartech PP5312 Mica Reinforced Homopolymer Information provided by Spartech |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Spartech Royalite R21 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Techmer ES HiFill® PP 0096 S3 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Techmer ES Plastiblend® ABS IM Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPallets.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 5102KR Cast Film Polypropylene HomopolymerApplications: Biaxially oriented film.Formolene 5102KR is a highly isotactic polypropylene homopolymer designed primarily for cast film applications such as slit tape fabric stock and cor.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite Butyrate 285A2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPP 200-4 PP Black Polypropylene Copolymer, No Break AAROLENE® ARPP 200-4 Series Polypropylene Compounded ResinFeatures: A copolymer polypropylene resin, pre-colored black, featuring excellent toughness for all extrusion applications. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D-638 |
Bapolene® 4072 Polypropylene, Injection Grade Bapolene PP4072 is a high flow, fast cycle injection molding resin. This product meets FDA standards for food contact applications.Applications: Appliances, containers, and thin-walled articles.Bap.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | |
Asahi Kasei Thermylene® P-20TC-1156 Chemically Coupled Polypropylene Compound, 20% Talc Filled Applications: Automotive: Blower Wheels, HVAC Electrical and Specialty: Flush Valves, Pump BasesInformation provided by Asahi Kasei |