Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
PolyMirae Moplen EP400M Injection Molding Grade Polypropylene Moplen EP400M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP400M is a block copolymer selected by customers for use in in.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
PolyMirae Moplen EP500N Injection Molding Grade Polypropylene Moplen EP500N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP500N is a block copolymer particularly suitable for injection.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CR020N Polypropylene Random Copolymer COPYLENE® CR020N is a random copolymer formulated with advanced nucleator technology and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have exceptional gloss a.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
Reliance Industries Repol B030MG Polypropylene REPOL Polypropylene B030MG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
Reliance Industries Repol C015EG Polypropylene REPOL Polypropylene C015EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | ASTM D638 |
M. Holland Company CP100 Polypropylene Impact Copolymer Impact copolymerHigh impact resistanceLow temperature impact resistanceApplications: PipingSheetInformation provided by M. Holland |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
Hyosung Topilene C600M3 PP C600M3 Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
Hyosung Topilene J340 PP J340 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation |
|||
Tensile Strength, Yield | 26.5 MPa @Thickness 3.20 mm |
3840 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
Tensile Strength, Yield | 26.5 MPa @Thickness 3.20 mm |
3840 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer SEETEC M1500 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1500 exhibits a high flowability and a good balance of stiffness and impact strength. SEETEC M1500 .. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer Features: SEETEC M1600 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1600 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
LG Chemical SEETEC PB270 HDPE Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplicatio.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
LG Chemical SI-610 Alphalac Polystyrene High flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include big size electric app.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
Lotte Chemical Titan TITANZEX® HB6200 High density polyethylene HB6200 is a high density polyethylene for blow molding. HB6200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. Applic.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
LG Chemical 40 AF Flame Retardant HIPS High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VT.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
LG Chemical 60HR-G HIPS High flow, Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape reco.. |
|||
Tensile Strength, Yield | 26.5 MPa @Thickness 3.20 mm |
3840 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
SCG Chemicals EL-Proâ„¢ P440J Polypropylene Injection Molding Key Characteristics:Excellent impact strengthSuitable for small to medium partsRecommended Applications:High impact and durable automotive, motorcycle and electrical appliance parts such as fan stan.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
Tipco Tipcolene® FPZ-GC - Talc/Mineral Reinforced Polypropylene Copolymer, High Flow, Stiffness & Impact Strength Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | |
Zylog Hipolyene® 9011 UHF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Tensile Strength, Yield | 26.5 MPa | 3850 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50mm/min; ASTM D638 |
LG Chemical SEETEC R7700 Polypropylene, Random Copolymer Features: Seetec R7700 is designed for the extrusion of fibers with the spunbond technology. This grade is characterized by narrow MWD and good processability. SEETEC R7700 meets the FDA requirement.. |
|||
Tensile Strength, Yield | 26.5 MPa | 3840 psi | ASTM D638 |
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical .. |