Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Multibase Multi-Pro® 3014 XUGW Polypropylene Mineral Filled.Features:Gloss, HighUV Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Multibase |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Maxxam™ SY 89-21-1 Polypropylene, Unspecified (PP, Unspecified) Maxxam ™ SY 89-21-1 is a polypropylene copolymer compound with a pre-dispersed blowing agent for up to 50% expansion. The compound offers consistent cell structure, dielectric properties, and stren.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Maxxam™ SY 89-23-7 Polypropylene, Unspecified (PP, Unspecified) Maxxam ™ SY 89-23-7 is a polypropylene copolymer compound with a pre-dispersed blowing agent for up to 60% expansion. The compound offers consistent cell structure, dielectric properties, and stren.. |
|||
Tensile Strength, Yield | >= 23.4 MPa | >= 3400 psi | ASTM D638 |
S&E Specialty Polymers TufGuard M™ GPP1005M-EXLT PP, Flame Retardant Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Entec Hypel® PEHD32/.951 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | Compression Molded; ASTM D638 |
NOVA Chemicals Surpass® RMs244-U Octene sHDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Standards 1.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 17% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
LyondellBasell Alathon® L5040 High Density Polyethylene, Blow Molding/Extrusion Grade Alathon L5040 is able to incorporate high levels of post consumer recycle and retain excellent bottle physical properties. This resin provides high ESCR and processing stability. Typical application.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Global PCC-0310 Standard Grade Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | 2 in/min.; ASTM D638 |
Ineos K46-06-185 HDPE K46-06-185 is a natural high molecular weight, high-density copolymer polyethylene developed for automotive fuel tanks. It combines excellent processability and outstanding physical performance, par.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Ineos L70Z-01 Polypropylene Impact Copolymer L70Z-01 is a nucleated and antistatic high flow polypropylene medium impact copolymer for injection molding applications. This product meets the requirements of the U.S. Food and Drug Administration.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Techmer ES HiFill® HIPS 484 GY Availability: North AmericaForms: PelletsAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Techmer ES HiFill® HIPS LE BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 8813148Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Spartech EP6240 Filled and Reinforced Copolymer Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D 638 |
Styrolution Zylar 960 MBS ZYLAR 960 is an impact modified styrene acrylic copolymer that provides toughness equivalent to some grades of polycarbonate, good clarity and superior processing characteristics for demanding injec.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Techmer ES HiFill® HIPS BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | press cure 11 min./160ºC |
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | after 7 days at 100ºC |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 1.5 PHR Sulfur MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | 2.0 in/min; ASTM D638 |
ExxonMobil HDP8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Tensile Strength, Yield | 23.4 MPa | 3390 psi | |
Dow HDPE 10462N High Density Polyethylene DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability.. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | 50 mm/min; ASTM D638 |
Amco PRIMATOP PP CO 350-20 Impact Polypropylene Copolymer PP CO 350-20 has easy mold flow and excellent dimensional stability. It is used in thin walled injection molded applications.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Tensile Strength, Yield | 23.4 MPa | 3400 psi | ASTM D638 |
Amco Amalloy® B1017 Polymer Alloy Amco Amalloy B1017 is a clear performance copolymer with exceptional clarity and toughness.High melt-flow, very clear.Information provided by Amco Plastic Materials. |