Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO 527 |
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO 527 |
Murtfeldt Original Material ”S”® Green Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO 527 |
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, H OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, Q OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, SG OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO 527-1 |
Orbilan ORBILAN® PE 1000 UHMW-PE Orbilan PE 1000 plastics distinguish themselves through their optimal balance of the technical features with regard to wear-resistance and impact resistance. The areas of use range from general mac.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D412 |
Precision Polymer Engineering R50Z Natural Rubber Natural Rubber, 45-55 °IRHD. Formulated to meet BS1154 Grade Z50. In accordance with BS1154 this material is based on high-quality plantation (Hevea) rubber, reinforced with carbon black.Applicati.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-2/1A |
Polymer Industries Polyslick UHMW Sheet Polyslick UHMW Sheet exhibits the properties of excellent impact strength, abrasion resistance, low coefficient of friction, as well as very good chemical resistance. This industrial grade material .. |
|||
Tensile Strength, Yield | >= 17.0 MPa | >= 2470 psi | ISO/R 527 |
Okulen® 2000 PE-UHMW, CL OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistati.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers SEQUEL® 1405 TPO
(discontinued **) Description: SEQUEL® 1405 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, high flow and e.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 110-1328 LMDPE Rotational Molding Resin Description: ICORENE 110-1328 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 115-1323 LMDPE Rotational Molding Resin Description: ICORENE 115-1323 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Kostat BK-STAT BK-STAT is an inherently dissipative polymer incorporated into a variety of resins as a melt additive. The electrical resistivity is reduced by formation of a conductive percolating network in the .. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
LG Chemical LUPOL TE-5102 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Impact LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
SCG Chemicals EL-Leneâ„¢ M3204 Butene (C4) Rotational Molding Resin Natural base resin available in pellet / powder formKey Characteristics:Low warpageGood processingGood impact resistanceTypical Applications:Low temperature service parts, straight-wall or flat-surf.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | 2 in/min, Type IV bar; ASTM D-638 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 100 % |
2470 psi @Strain 100 % |
ISO 527-1/-2 |
Covestro Desmopan® W DP 89051D Polyurethane PreprocessingMax. Water content |
|||
Tensile Strength, Yield | 17.0 MPa @Strain 50.0 % |
2470 psi @Strain 50.0 % |
|
Covestro Texin® 390 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-2 |
ExxonMobil Exxtral™ BMU 139 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ BNT 011 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior parts such as bumper fascia.Availability: Africa & Middle East, Asia Pacific,.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO 527-2/50 |
ExxonMobil Exxtral™ H1725W Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with very high flow. Product presenting very high rigidity, maintaining excellent impact resistance properties, including at a low tem.. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0437W20L1 Wollastonite Reinforced |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | |
BASF Polystyrol® 2712 Impact Grade Polystyrene (Europe) Easy flowing special grade, particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 17.0 MPa | 2470 psi | ISO R527-1 |
LyondellBasell Hifax™ ETA-3163 Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good dimensional stability, good paintability, good pro.. |