Polymer Property : Film Tensile Strength at Break, MD = 6240 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ISO 527-3
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene
Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:..
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ASTM D882
NOVA Chemicals Sclair® 12J1 Octene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, high clarity.Applications: Overwrap, lamination.Data provided by the manufacturer.
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ASTM D882
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st..
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ASTM D882
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene
12XF6 is a high performance LLDPE (HP-LLDPE) blown film grade for high film strength applications.Information provided by Iran Petrochemical Commercial Co.
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ASTM D882
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene
235F7 is a LLDPE blown film grade designed for general purpose film application. This resin is particularly suited for blending with LDPE, giving better strength and downgauging possibility.Informat..
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ASTM D882
Chevron Phillips MarFlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film
This LLDPE is tailored for cast film applications that require:Good stiffness at thin gaugesGood drawdownExcellent processabilityCan be used singly or in blends with LDPE or HDPEAvailable with slip ..
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
Cast Film at 1.25 mil; ASTM D-882
Chevron Phillips MarFlex® 7120X Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L..
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ASTM D882
NOVA Chemicals Surpass® FPs117-D Octene sLLDPE Film Resin  (discontinued **)
Applications: Lamination Film, coextruded sealant layer, high toughness filmInformation provided by Nova Chemicals
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ASTM D882
NOVA Chemicals Sclair® 11G1 LLDPE Film Resin  (discontinued **)
Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionAdditives: Process stabilizer, Polymer process aidFilm properties are typical of blown film..
Film Tensile Strength at Break, MD 43.0 MPa
6240 psi
ASTM D882
NOVA Chemicals Sclair® 11N1 PE Film Resin  (discontinued **)
Low gel, Excellent seal characteristics, Easy processabilityApplications: Premium shrink film, Co-extrusionFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are depe..