Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
DuPont™ Surlyn® NWL Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® NWL is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Film produced from this resin is .. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | MD-TD Average; ASTM D882 |
DuPont Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film 15 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | D638 |
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength m.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
Westlake EF606 Low Density Polyethylene Westlake EF606 is a LDPE resin suggested for use in multiwall and general purpose liners, and for use as a blend resin in general purpose packaging applications. It has excellent processability, and.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
Westlake EF706 Low Density Polyethylene Westlake EF706 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
Formosa Plastics Formolene® L42022B Film (Butene Grade) LLDPE Butene Copolymer (Barefoot)Applications: Blown and cast filmBlown and cast filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of p.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
Formosa Plastics Formolene® L42022E2 Film (Butene Grade) LLDPE Butene Copolymer (Low slip and antiblock)Applications: Thin gauge blown filmThin gauge blown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, cove.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LD 124.MS General Purpose Clarity Film Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil Escorene® LD 720.01 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
ExxonMobil Escorene® LD 720.62 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D-882 |
Bapolene® 222F Polyethylene, Film Grade Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/a.. |
|||
Film Tensile Strength at Break, MD | 26.9 MPa | 3900 psi | ASTM D882 |
DuPont™ Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1652SB is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |