Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 100 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 125 BSR-ONE OPP Film Product Description: Bicor BSR-ONE is a two-side sealable, one side treated, coextruded OPP film designed for unsupported plain or surface print applications, and in laminations on both HFFS and VF.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | ExxonMobil Method |
ExxonMobil Bicor® 150 ASB-X OPP Film Product Description: Bicor ASB-X is a two side coated, sealable OPP film designed for broad use in many applications, including overwrap, horizontal, and vertical packaging. This film is suitable as.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 60 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 70 HSH OPP Film Product Description: Bicor HSH is a one-side treated, one-side sealable, coextruded OPP film designed for use in unsupported plain or surface print high-speed horizontal applications.Availability: .. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 75 AB-X OPP Film Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 75 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 75 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 18 LPX-2 OPP Film Product Description: Bicor LPX-2 is a one-side treated, one-side sealable OPP film designed for use in a lamination. It can be laminated to Metallyte, HBS-2, and itself to create lap sealable packag.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor™ 60 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |
|||
Film Tensile Strength at Break, MD | 124.11 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte® 15 LLG-101 Clear OPP Film Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (and other gauges of LLF-101) or applied.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte® 19 LLG-101 Clear OPP Film Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied .. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte® 25 LLG-101 Clear OPP Film Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied .. |
|||
Film Tensile Strength at Break, MD | 124.11 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte® 30 LLG-101 Clear OPP Film Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied .. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 19LL-101 OPP Film Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling appl.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 25LL-101 OPP Film Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling appl.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL-101 OPP Film Product Description: A clear, one-side treated, polypropylene film that is designed to provide exceptional clarity and print protection when used as overlaminates in pressure-sensitive labeling appl.. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 7.9 in/min, 4.9 in Jaw Separation; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM882 OPP Film Product Description: An ultra high barrier (UHB), biaxially oriented, multilayer polypropylene film. In addition to an excellent water vapor barrier, this film has an exceptional barrier to oxygen, .. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 120 CSR-2 OPP Film Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and .. |
|||
Film Tensile Strength at Break, MD | 124 MPa | 18000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 120 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |