Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Yield, MD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
Film Tensile Strength at Yield, MD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Yield, MD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil Enable™ 27-05CH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-05CH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Yield, MD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin Product Description: Enable 27-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |
|||
Film Tensile Strength at Yield, MD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
Film Tensile Strength at Yield, MD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade) Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No.. |
|||
Film Tensile Strength at Yield, MD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A.. |
|||
Film Tensile Strength at Yield, MD | 13.1 MPa | 1900 psi | ASTM D882 |
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin (European Grade) Product Description: Enable 27-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and .. |