Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 197 Polyester Film Melinex® 197 is a very clear polyester film with good handling properties, suitable for general purpose applications.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 313 Polyester Film Melinex® 313 is a general purpose polyester film with consistently good handling properties. It is pretreated on one side for adhesion.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 314 Polyester Film, 200 Gauge Melinex® 314 is a two-side adhesion promoting polyester film with consistently good handling properties.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 314 Polyester Film, 92 Gauge Melinex® 314 is a two-side adhesion promoting polyester film with consistently good handling properties.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 376 Polyester Film Melinex® 376 is a translucent, smooth, matte polyester film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Information provided by DuPont. |
|||
Film Tensile Strength at Yield, MD | 100 MPa @Strain >=5.00 % |
14500 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 142 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, MD | 100 MPa @Strain >=5.00 % |
14500 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 200 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, MD | 100 MPa @Strain >=5.00 % |
14500 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 300 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, MD | 100 MPa @Strain >=5.00 % |
14500 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 48 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, MD | 100 MPa @Strain >=5.00 % |
14500 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 500 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, MD | 100 MPa @Strain >=5.00 % |
14500 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 75 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, MD | 100 MPa @Strain >=5.00 % |
14500 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 377 Polyester Film, 92 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 515 Polyester Film A high clarity film which is two side pretreated for slip to combine good handling properties with high clarity and brilliance.Typical Applications: MELINEX® 515 is suitable for applications which .. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 581 Polyester Film A super clear, one side C-Sub pretreated film for adhesion of hydrophilic coatings.Approvals: UL Recognition - Product has been registered with Underwriters LaboratoriesInformation provided by DuPon.. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® 582 Polyester Film, 400 Gauge Melinex® 582 is a high clarity polyester film which is two-side hydrophilic pretreated to promote adhesion to many industrial aqueous coating and inks.Approvals: UL Recognition - Product has been r.. |
|||
Film Tensile Strength at Yield, MD | 100 MPa @Strain >=5.00 % |
14500 psi @Strain >=5.00 % |
ASTM D882A |
DuPont Teijin Films Melinex® 583 Polyester Film, 300 Gauge Melinex® 583 is a high clarity, differentially treated polyester film. One side is hydrophilic pretreated to promote adhesion to many industrial aqueous coatings and inks, and the opposite side is .. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 200 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 300 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 400 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 92 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 142 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Film Tensile Strength at Yield, MD | 100 MPa | 14500 psi | ASTM D882A |
DuPont Teijin Films Melinex® S Polyester Film, 75 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |