Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 21.0 MPa | 3050 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PE 1271 PRE-ELEC PE 1271 is a conductive thermoplastic compound based on a blend of PE-LD/PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivi.. |
|||
Film Tensile Strength at Yield, MD | 21.0 MPa | 3050 psi | ASTM D882 |
Polymer Industries Densetec HDPE Rod Polymer Industries’ HDPE Rod exhibits all the durable qualities found in Densetec HDPE Sheet, making it perfect for that industrial application where sheet stock is not suitable. The HDPE Rod is av.. |
|||
Film Tensile Strength at Yield, MD | 21.0 MPa | 3050 psi | ASTM D882 |
NOVA Chemicals Sclair® 15A Butene HDPE Film Resin Film Properties. Features: Low gel, good barrier properties, strength and toughness.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 21.0 MPa | 3050 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PE 1308
(discontinued **) PRE-ELEC PE 1308 is a conductive thermoplastic compound based on a blend of PE-LD/PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivi.. |
|||
Film Tensile Strength at Yield, MD | 21.0 MPa | 3050 psi | ASTM D882 |
Eastman D4028-F Polyethylene
(discontinued **) D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF.. |
|||
Film Tensile Strength at Yield, MD | 21.0 MPa | 3050 psi | ASTM D882 |
Eastman E6838-014F Polyethylene
(discontinued **) E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta.. |
|||
Film Tensile Strength at Yield, MD | 21.0 MPa | 3050 psi | ASTM D882 |
NOVA Chemicals Sclair® 16A Butene HDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good barrier properties.Applications: Merchandising bags, lamination, co-extrusion.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 21.0 - 22.0 MPa | 3050 - 3190 psi | Average value: 21.3 MPa Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim.. |
|||
Film Tensile Strength at Yield, MD | 21.0 - 35.0 MPa | 3050 - 5080 psi | Average value: 28.9 MPa Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |