Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
ExxonMobil Enable™ 27-03CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-03HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
ExxonMobil Enable™ 27-05CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-05CH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin
Product Description: Enable 27-05HH is a metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin
Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi..
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade)
Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No..
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
ExxonMobil Nexxstar™ NX-00328 Low Density Polyethylene Resin
Product Description: Nexxstar 00328 is an LDPE grade, which offers good film rigidity combined with very good optical properties. Its primary use is for high performance collation shrunk packaging.A..
Film Tensile Strength at Yield, MD 13.1 MPa
1900 psi
ASTM D882
ExxonMobil Enable™ 27-05HH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-05HH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Copyright © lookpolymers.com All Rights Reserved