Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
SABIC 518N Linear Low Density Polyethylene for Blown Film Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 24 Low Density Polyethylene - Blown Film Extrusion Riblene FL 24 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 24 is characterized by a good balance between processabilit.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-0718-A LDPE Film Resin Improves gloss and reduces haze in blends with LLDPE, Improves melt strength and increases output in blends with LLDPEApplications: Blends with LLDPEAdditives: Base resinFilm properties are typical .. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 I is recommended for the .. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527 |
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y819-C LDPE Film Resin Film Properties. Features: Good strength and toughness, excellent shrink film characteristics, excellent processability.Applications: Industrial packaging, liners, shrink film, blends with LLDPE.Da.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-B Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Trash bags, liners, general packaging.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Industrial liners, heavy duty bags.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
NOVA Chemicals Novapol® PF-0118-F Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Stretch wrap, blend resin, industrial packaging.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Montell 16501F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Montell 16501F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Montell 16502F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
LyondellBasell Montell 16502F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527 |
Iran Petrochemical (PCC) LH0030 Low Density Polyethylene LH0030 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Applications: general packaging applications, part.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 can be processed at high outpu.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film LL 1820 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 H can be processed at high o.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ISO 527-3 |
Total LLDPE LL 1820 Linear Low Density Polyethylene - Blown Film LL 1820 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1820 can be processed at high outpu.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LD 071.LQ Blown Film Resin L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | |
Dow DOWLEX™ 2045.02 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2045.02 Polyethylene resin is a premier film resin for general packaging applications ranging from heavy duty applications to high speed, thin gauge applications. It contains high level of .. |
|||
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
Dow DOWLEX™ 2020G Linear Low Density Polyethylene DOWLEX™ 2020G is perfect for high strength consumer trash bags/liners. This product can be used in other applications that require toughness and also offers great melt strength for high throughput.. |