Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 200 MPa @Strain 1.00 %, Temperature 300 °C |
29000 psi @Strain 1.00 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 200 MPa @Strain 1.00 %, Temperature 300 °C |
29000 psi @Strain 1.00 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 200 MPa @Strain 0.200 % |
29000 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 200 MPa @Strain 0.200 % |
29000 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 200 MPa @Strain 1.00 %, Temperature 300 °C |
29000 psi @Strain 1.00 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Tensile Strength, Yield | 200 MPa @Strain 0.200 % |
29000 psi @Strain 0.200 % |
EN min.,RT; EN 10002-1 |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Tensile Strength, Yield | 200 MPa @Strain 0.200 %, Temperature -80.0 °C |
29000 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Tensile Strength, Yield | >= 200 MPa @Temperature 100 °C |
>= 29000 psi @Temperature 212 °F |
|
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength, Yield | >= 200 MPa @Strain 0.200 % |
>= 29000 psi @Strain 0.200 % |
|
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi.. |
|||
Tensile Strength, Yield | >= 200 MPa @Strain 0.200 % |
>= 29000 psi @Strain 0.200 % |
|
Industeel CLC 18.10 Nb Niobium Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Nb is a 18Cr-10Ni austenitic stainless steel stabilized with specific Nb addition. This kind of steel is one of the basic grades of the stainless steels range. Niobium bearing and its low c.. |
|||
Tensile Strength, Yield | >= 200 MPa @Strain 0.200 % |
>= 29000 psi @Strain 0.200 % |
|
Industeel CLC 18.10Ti Titanium-Stabilized 18Cr-10Ni Austenitic Stainless Steel CLC 18-10Ti is a 18Cr-9Ni austenitic stainless steel stabilized with some Titanium additions. This is a basic grades in the stainless steel range. Titanium bearing (carbide forming element) avoids i.. |
|||
Tensile Strength, Yield | >= 200 MPa @Strain 0.200 % |
>= 29000 psi @Strain 0.200 % |
|
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k.. |